Metallographic Etchants - Zinc

Metallographic Etchants

Zinc Alloy Etchants

CAUTION: Safety is very important when etching. Be sure to wear the appropriate protective clothing and observe all WARNINGS on chemical manufacturers MSDS. Also review COMMENTS Section for each etchant.

Etchant

Conc.

Conditions

Comments

Distilled water or Ethanol
Hydrochloric acid

100 ml
1-5 ml

Several minutes

Zinc and zinc alloys

Distilled water
Sodium Hydroxide

100 ml
10 grams

 1-5 seconds

Low alloy zinc and pure zinc

Distilled water
CrO3
Na2SO4

100 ml
20 grams
1-5 grams

Seconds

Swabbing


Metallographic micrograph of etched zinc-aluminum alloy
Zinc-aluminum alloy, 200X B.F., (etchant CrO3, Na2SO4)