Data Storage - Corrosion Inhibitors

Copper GMR Corrosion

Copper Pourbaix Diagram

GMR copper corrosion

Corrosion Potentials:
The Pourbaix diagram indicates that below a pH of 7 and at higher oxidation potential, copper can corrode. Since D.I. water typically has a pH value less then 6 and has an oxidation range in the vicinity of Cu(+2), thermodynamically copper can corrode.

Corrosion Rates:
The Tafel plots show that with the addition of a corrosion inhibitor, the corrosion rate of cobalt can be reduced from 1.76 angstroms/minute to 0.0026 Angstroms/minute.

GMR copper corrosion