Data Storage - Corrosion Inhibitors

Manganese GMR Corrosion

Manganese Pourbaix Diagram

GMR manganese corrosion

Corrosion Potentials:
The Pourbaix diagram indicates that the corrosion potential of manganese is very pH dependent. For pH values below 11 manganese can thermodynamically form a Mn(+2), which is a corrosion product of manganese. Since D.I. water typically has a pH value less then 6, manganese is very suceptible to cleaning and water based lubricants or slurries. Above a pH of 11, manganese can form both stable oxides and a manganese hydroxide ion, so passivating manganese is very dependent upon the solution chemistry.

Corrosion Rates:
The Tafel plots show that with the addition of a corrosion inhibitor, the corrosion rate of managanese can be reduced from a very high level of 124.1 angstroms/minute to a more acceptable level of 2 Angstroms/minute at even very low additions of an organic corrosion inhibitor. The corrosion value can be reduced further with higher concentrations of the organic inhibitor.

GMR manganese corrosion
GMR manganese corrosion

About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2006
PACE Technologies - 1802 W. Grant Rd. No. 102 - Tucson, AZ 85745 USA
Telephone 520-882-6598 FAX 520-882-6599.
All Rights Reserved.