Data Storage - Corrosion Inhibitors

Tantalum GMR Corrosion

Tantalum Pourbaix Diagram

GMR tantalum corrosion

Corrosion Potentials:
The Pourbaix diagram indicates that tantulum does not form any corrosive ions within the stability region of water. Therere, D.I. water cannot thermodynamically corrode tantulum.