DVD / CD Scratch Repair - Polishing Abrasives

DVD / CD Polishing Abrasives

Alumina Polishing Abrasives

There are a number of different types of alumina polishing abrasives. These abrasive are classified by there manufacturing process, crystal structure (hardness) and their classification process. The main types of alumina’s produced for polishing are either calicned or polycrystalline alumina. Calcined powders can also be characterized as either fused, platey or levigated (air classified / sized) alumina depending upon the grain shape, purity and classification process. There is a major difference in the performance between calcined and polycrystalline alumina abrasives, especially for the submicron particle sizes. The two common crystal structures are the harder alpha alumina (mohs hardness 9) and the softer gamma crystal structure (mohs hardness 8).

Alumina Slurry / Suspensions

Alumina
Type
Crystal
Hardness
Particle Size
(microns)
Part Number
Calcined
Alpha
9
0.50
1.0
3.0
5.0
NANO-1050
NANO-1100
NANO-1300
NANO-1500

About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2006
PACE Technologies - 1802 W. Grant Rd. No. 102 - Tucson, AZ 85745 USA
Telephone 520-882-6598 FAX 520-882-6599.
All Rights Reserved.