Technical Information - Polycrystalline Diamond

Polycrystalline Diamond Polishing Abrasives

Polycrystalline Diamond

Polycrystalline diamond abrasives are manufacturered by transforming graphite into diamond via a high temperature and high pressure explosion process. The resulting particle is comprised of numerous microcrystallites bonded together. Particle sizing is accomplished by milling or grinding the aggregate particle.

 
HSEM (High Resolution Scanning Electronic Microscope) picture of our powder size 0.05-.2 mcm at 10,000 times magnification.   HSEM (High Resolution Scanning Electronic Microscope) picture of our powder size 0.05-.2 mcm at 600,000 times magnification.

Polycrystalline diamond as compared to synthetic and natural monocrystalline diamond provides better surface finishes and higher removal rates for metallographic specimen preparation. The features and advantages of polycrystalline diamond include the following:

  • Higher cutting rates
  • Very uniform surface finish
  • More uniform particle size distribution
  • Higher removal rates (self sharpening abrasives)
  • Harder/tougher particles
  • Blocky shaped
  • Hexagonal microcrystallites (equally hard in all directions)
  • Extremely rough surface (more cutting points)
  • Surface area 300% greater than monocrystalline diamond
  • No abrasion-resistant directionality (abrasion independent of particle orientation)

Polycrystalline Diamond Technical data

Appearance (dry state):

Color

Gray

Chemical composition:

Carbon

99 %

Hydrogen

< 1 %

Nitrogen

< 1%

Oxygen

< 1%

Physical data:

Particle sizes available:

0.05-0.15; 0.05-0.2; 0-0.25; 0-0.5; 0.5-1.0; 0-1.0; 0.5-1.5; 1-2; 0-2; 1-3; 0-10 um.

Specific gravity:

3.451

Friability index:

75-80%

Structure:

polycrystalline, with the block size under 0.1 um

Decomposition

decomposes with a heat over 500°C

Electrical conductivity:

non-conductive



Recommended Application

The following is a list of recommendations to maximize the performance of the polishing or lapping operations.

  • Match the polishing pad characteristics to the material to be polished
  • Charge diamond at higher pressure than the lapping process
  • Use a polishing lubricant designed to remove polishing or grinding swarf. This can significantly increase the life and performance of the polishing surface

About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2006
PACE Technologies - 1802 W. Grant Rd. No. 102 - Tucson, AZ 85745 USA
Telephone 520-882-6598 FAX 520-882-6599.
All Rights Reserved.