Description

Speed (rpm)

Base Polisher

Catalog Number

FEMTO-1000

0-200 rpm (variable)

NANO 1000/2000 (required)

FEMTO-1000

FEMTO-2000 (under development)

0-500 rpm

NANO 1200/2200 (required)

FEMTO-2000

Return to top



Individual FEMTO 1000 Automated Grinder/Polishers (with variable speed control)

 

Feature

Description

Application of Force

Individual

Head speed

0-200 rpm (variable)

Samples

1-6

Force

1.1 lbs to 13.5 lbs
(5N to 60N)

Compatibility

NANO series polishers

Construction

GRP (glass reinforced plastic)

Voltage

110V/220V, 50/60 Hz

Dimensions (WxHxL)

13" x 18" x 18"

Weight

55 lbs (25 kg)



Automated metallographic polisherFEMTO autopolishing head demoFEMTO 1000 autopolisher demo
 
Automated metallographic polisher
 

Accessories for FEMTO 1000 Automated Polishing Heads

Specimen Holder

Part Number

Single specimen holder mounting fixture for FEMTO 1000, includes one set of 6 each 1-inch, 1.25-inch and 1.5-inch plastic rings

SH-1100

1-in diameter rings

SR-0100

1.25-in diameter rings

SR-0125

1.5-in diameter rings

SR-0150

2-inch single specimen holder mounting fixture for FEMTO 1000, includes one set of 3, 2-inch plastic rings

SH-1200

2-in diameter specimen rings - requires SH-1200

SH-0200

Air filter / lubricator for compressed air AIR-0100
Plastic lubricator reservoir bottle LUB-1000

Return to top


Individual / Central FEMTO 2000 Automated Grinder/Polishers (with variable speed control) - under development

 

Feature

Description

Application of Force

Individual / Central

Head speed

0-500 rpm, contra or complimentary

Samples

Central 3-10 samples
Individual 1-8 samples

Force

Central 11.25 to 81 lbs
Individual 1.1 to 13.5 lbs

Controls

Microprocessor with touch pad

Construction

GRP (glass reinforced plastic)

Voltage

110V, 60 Hz

Dimensions (WxHxL)

16" x 24" x 18"

Weight

105 lbs



Automated metallographic polisherDIGIPREP Polisher Demo

 

 

 

Accessories for FEMTO-2000 Automated Polishing Heads

Central specimen holder for 12/14-inch polishers (8-inch outside diameter of holder)

Description

Part Number

1-inch diameter holder for 3 to 10 specimens

CT-2100

1.25-inch diameter holder for 3 to 8 specimens

CT-2125

1.5-inch diameter holder for 3 to 6 specimens

CT-2150

2-inch diameter holder for 3 specimens

CT-2200

Blank holder SR-B
Specimen loading plate for central pressure holder LP-0800

Individual Specimen holders for FEMTO 2000 Automated Polishing Heads

Specimen Holder

Part Number

Single specimen holder mounting fixture for FEMTO 1000, includes one set of 6 each 1-inch, 1.25-inch and 1.5-inch plastic rings

SH-2200

1-inch diameter rings

SR-2100

1.25-inch diameter rings

SR-2125

1.5-inch diameter rings

SR-2150

2-inch diameter rings (4 rings)

SR-2200

Blank holder

33-06


Return to top


About Us | Site Map | Web Disclaimer| Terms and Conditions| Contact Us

Copyright © 2011
PACE Technologies - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.