Microhardness Testers
Precision microhardness testing instrument for Vickers and Knoop indenters.

The MHV-2000 microhardness testers include a large LCD screen for displaying measuring methods, testing force, indentation length, hardness value, dwell time and the number of measurements. The MHV-2000 microhardness testers are available with a manual or an auto-turret and have a testing force ranging from 10 grf to 2000 grf.

The HVS-1000Z is an excellent microhardness tester at a great price. The HVS-1000Z has a automated turret to protect the indenter from being damaged by automatically moving it during after and before the loading and unloading cycles. The load range for the HVS-1000 is variable up to 1000 grf.

Microhardness testers  

Feature

HVS-1000Z

MHV-2000

MHV-2000A

Objective/ Indenter

Auto Turret

Manual Turret

Auto Turret

Testing force (gf)

10, 25, 50, 100, 200, 300, 400, 500, 1000

10, 25, 50, 100, 200, 300, 400, 500, 1000, 2000

10, 25, 50, 100, 200, 300, 400, 500, 1000, 2000

Indenter measurement

HRA, HRB, HRC, HV, HK, HBW

HRA, HRB, HRC, HV, HK, HBW

HRA, HRB, HRC, HV, HK, HBW

Objective magnification

10X, 40X

10X, 40X

10X, 40X

Testing range

1 HV ~ 3000 HV

1 HV ~ 3000 HV

1 HV ~ 3000 HV

X-Y Anvil size 100 x 100 mm 100 x 100 mm 100 x 100 mm
Indentor Type Vickers or Knoop Vickers or Knoop Vickers or Knoop
Illumination Halogen Halogen Halogen
Maximum height of specimen 70 mm 70 mm 70 mm
Power 110 or 220V 110 or 220V 110 or 220V
Dimensions 420x180x470 mm
(16.5x7x18.5 in)
420x180x470 mm
(16.5x7x18.5 in)
420x180x470 mm
(16.5x7x18.5 in)
Weight 25 kg (55 lbs) 25 kg (55 lbs) 25 kg (55 lbs)
 
Metallographic Microhardness Tester
 

Return to top

About Us | Site Map | Web Disclaimer| Terms and Conditions| Contact Us

Copyright © 2011
PACE Technologies - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.