Metallographic Rockwell and Superficial Rockwell Testers

Click here to get a quote
Hardness Tester Rockwell Superficial
Rockwell
Dual Superficial
Rockwell
Manual OMEGA-RT OMEGA-ST  
Standard OMEGA
RT-60/150
  OMEGA
SRT-15/150
Semi-automated OMEGA
DIGI-RT
  OMEGA
DIGI-RST
Automated OMEGA
AUTO-RT
OMEGA
AUTO-ST
OMEGA
AUTO-RST

Rockwell Hardness Testers

Manual Rockwell Hardness Tester (OMEGA-RT)

The OMEGA-RT is a basic low cost manual Rockwell hardness tester (Part No. OMEGA-RT) designed to evaluate metallographic specimen hardness.
Manual Rockwell hardness tester

Feature

OMEGA-RT

Rockwell Scales

HRA, HRB,HRC

Preliminary test force

10 Kgr (98.07N)

Full test force

60 Kgf, 100 Kgr, 150 Kgf

Loading control

manual

Instrument Throat Height 6.5-inch (165 mm)
Dimensions (W x D x H) 7.2 x 21.5 x 29.7 inch (182 x 546 x 755mm)
Weight 200 lbs (90 kg)
Accuracy Conforms to ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote

Return to top

Digital Rockwell Hardness Tester (OMEGA-RT-60/150)

The OMEGA-RT-60/150 is a semi-automated digital Rockwell hardness tester (Part No. OMEGA-RT-60/150) designed to evaluate metallographic specimen hardness.
Rockwell hardness tester

Feature

OMEGA-RT-60/150

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

10 Kgr (98.07N)

Full test force

60 Kgf, 100 Kgr, 150 Kgf

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRA, HRB, HRC, HRF, HV, HK, HBW, HT15N, HR30N, HR45N, HR15T, HR30T, HR45T
Illumination Halogen (LED optional)
Instrument Throat Height 6.3-inch (160 mm)
Power 110 or 220V
Dimensions (W x D x H) 8.5 x 20 x 28 inch (216 x 508 x 711mm)
Weight 200 lbs (90 kg)
Accuracy Conforms to ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote
 

Return to top

Digital Semi-Automated Rockwell Hardness Tester (OMEGA-DIGI-RT)

OMEGA-DIGI-RT is a semi-automated digital Rockwell hardness tester The OMEGA-DIGI hardness testers are designed to evaluate metallographic specimen Rockwell hardness.
Rockwell hardness tester

Feature

OMEGA-DIGI-RT

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

10 Kgr (98.07N)

Full test force

60 Kgf, 100 Kgr, 150 Kgf

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HV, HBS, HBW, HK, HRA, HRD, HR15N, HR30N, HR45N, HS, HRF, HR15T, HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 7 x 21.5 x 30 inches
(182 x 546 x 755 mm)
Weight 265 lbs (120 Kg)
Accuracy Conforms to ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote
 

Return to top

Automated Rockwell Hardness Tester (OMEGA-AUTO-RT)

OMEGA-AUTO-RT is an automated digital Rockwell hardness tester The OMEGA-AUTO-RT hardness testers are designed to evaluate metallographic specimen Rockwell hardness.
Rockwell hardness tester

Feature

OMEGA-AUTO-RT

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

10 Kgr (98.07N)

Full test force

60 Kgf, 100 Kgr, 150 Kgf

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HV, HBS, HBW, HK, HRA, HRD, HR15N, HR30N, HR45N, HS, HRF, HR15T, HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 11 inches (280 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 275.6 lbs (125 Kg)
Accuracy Conforms to GB/T230.2, JJS Z2245, EN-ISO 6508, ASTM E-18
Metallographic Automated Rockwell Hardness Tester Click here to get a quote
 

Return to top


Superficial Rockwell Hardness Testers

Manual Superficial Rockwell Hardness Tester (OMEGA-ST)

The OMEGA-ST is a basic low cost manual Superficial Rockwell hardness tester (Part No. OMEGA-ST) designed to evaluate metallographic specimen hardness.
Manual Superficial Rockwell hardness tester

Feature

OMEGA-ST

Rockwell Scales

HR15N, HR30N, HR45N, HR15T, HR30T, HR45T

Preliminary test force

3 Kgf (29.4N)

Full test force

15 Kgf, 30 Kgr, 45 Kgf

Loading control

manual

Instrument Throat Height 6.5-inch (165 mm)
Dimensions (W x D x H) 7.2 x 21.5 x 29.7 inch (182 x 546 x 755mm)
Weight 200 lbs (90 kg)
Accuracy Conforms to ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote

Return to top

Automated Superficial Rockwell Hardness Tester (OMEGA-AUTO-ST)

OMEGA-AUTO-ST is an automated digital Superficial Rockwell hardness tester The OMEGA-AUTO-ST hardness testers are designed to evaluate metallographic specimen Superficial Rockwell hardness.
Superficial Rockwell hardness tester

Feature

OMEGA-AUTO-ST

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

3 Kgr (29.4N)

Full test force

15 Kgf, 30 Kgr, 45 Kgf

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HV, HBS, HBW, HK, HRA, HRD, HR15N, HR30N, HR45N, HS, HRF, HR15T, HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 11 inches (280 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 275.6 lbs (125 Kg)
Accuracy Conforms to GB/T230.2, JJS Z2245, EN-ISO 6508, ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote
 

Return to top


Dual Rockwell / Superficial Rockwell Hardness Testers

Digital Dual Rockwell / Superficial Rockwell Hardness Tester (OMEGA-SRT-15/150)

The OMEGA-SRT-15/150 is an automated digital Rockwell / Superficial Rockwell Testing machine (Part No. OMEGA-SRT-15/150) designed for evaluating metallographic specimen hardness.
Superficial Rockwell hardness tester

Feature

OMEGA-SRT-15/150

Rockwell Scales

HRA, HRB, HRC, HRD, HRE,
HRF, HRG,HRH, HRK, HRL,
HRM, HRR, HRP, HRS, HRV,
HR15N, HR30N, HR45N,
HR15T, HR30T, HR45T

Preliminary test force

3 Kgr (Superficial)
10 Kgr (Rockwell)

Full test force

15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HRB, HRA, HV
HK, HBW
Illumination Halogen (LED optional)
Instrument Throat Height 6.3-inch (160 mm)
Power 110 or 220V
Dimensions (W x D x H) 7 x 21.5 x 30 inches
(182 x 546 x 755 mm)
Weight 200 lbs (90 kg)
Accuracy Conforms to ASTM E-18
Metallographic Superficial Rockwell Hardness Tester Click here to get a quote
 

Return to top

Digital Semi-Automated Dual Rockwell/ Superficial Hardness Tester (OMEGA-DIGI-RST)

OMEGA-DIGI-RST is a semi-automated digital dual Rockwell/ Superficial Rockwell hardness tester. The OMEGA-DIGI semi-automated hardness testers are designed to evaluate metallographic specimen Rockwell and Superficial Rockwell hardness.
Rockwell hardness tester

Feature

OMEGA-DIGI-RST

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

3 Kgr (Superficial)
10 Kgr (Rockwell)

Full test force

15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HV, HBS, HBW, HK, HRA, HRD, HR15N, HR30N, HR45N, HS, HRF, HR15T, HR30T, HR45T, HRB
Illumination Halogen (LED optional)
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 265 lbs (120 Kg)
Accuracy Conforms to ASTM E-18
Metallographic dual Superficial and Rockwell Hardness Tester Click here to get a quote
 

Return to top

Digital Automated Dual Rockwell/ Superficial Hardness Tester (OMEGA-AUTO-RST)

OMEGA-AUTO-RST is an automated digital dual Rockwell/ Superficial Rockwell hardness tester. The OMEGA-AUTO-RST hardness testers are designed to evaluate metallographic specimen Rockwell and Superficial Rockwell hardness.
Rockwell hardness tester

Feature

OMEGA-AUTO-RST

Rockwell Scales

HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV

Preliminary test force

3 Kgr (Superficial)
10 Kgr (Rockwell)

Full test force

15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)

Hardness resolution

0.1 HR

Dwell time

Adjustable 1-60 seconds

Auto Hardness conversion HRC, HV, HBS, HBW, HK, HRA, HRD, HR15N, HR30N, HR45N, HS, HRF, HR15T, HR30T, HR45T, HRB
Illumination Halogen (LED optional)
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 265 lbs (120 Kg)
Accuracy Conforms to ASTM E-18
Metallographic Rockwell Hardness Tester Click here to get a quote
 

Return to top

About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us

Copyright 2006-2017
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1 520-882-6598 FAX +1 520-882-6599
All Rights Reserved


PACE Technologies facebook link   Blog us on Tumblr   Blog us on Tumblr   PACE Technologies Google+   PACE Technologies Google+   PACE Technologies Google+