PENTA-5000 5-Station Hand Grinder (NEW - BEST VALUE)

The PENTA-5000 5-station hand grinder (Part. No. PENTA-5000) offers a small lab the ability to prepare samples for macro viewing within minutes. The PENTA-5000 is a stationary grinder using 3-7/16 x 60-ft rolls set up for 240, 360, 600, 800 and 1200 grit abrasive.
Hand GrinderMetallographic Manual Hand Grinder Click here to get a quote
Feature Specification
Grinding stations 240, 360, 600, 800 and 1200 grit silicon carbide rolls
Roll sizes 3-7/16-inch width x 60 feet length with 1 -inch core
Construction -Aluminum casting and stainless steel
-Hard coat anodized rollers and paper support plates
Cooling rinse system Water
Dimensions
(W x D x H)
22.25 x 21 x 8 -inch
(565 x 535 x 203 -mm)
Weight 55 lbs (25 kg)

PENTA-7500 Belt Grinder (NEW - BEST VALUE)

The PENTA-7500 belt grinder (Part No. PENTA-7500) offers the ability to rapidly planarize a specimen or to grind it to the desired area of interest. The unique benefit the PENTA-7500 offers for planarizing specimen mounts, is especially useful for maintaining a square mount and minimizing the preparation time for automated polishing machines.
Microhardness testersMetallographicPENTA 7500 Belt Grinder Click here to get a quote
Feature Specification
Single belt 4 x 36-inch
(102 x 914 mm)
Electrical Specification 110V / 220V 50/ 60 Hz
Motor power 550 W (0.75 hp)
Cooling / rinse system Water
Construction Aluminum casting /
fabricated metal
Dimensions (W x D x H) 20 x 24.75 x 14.75 -inch
(510 x 630 x 375 mm)
Weight 120 lbs (53 kg)

PENTA-7500 Squaring Holder Sleeves

Accessories Part Number
1-inch sleeve for square holder (each) P75-100H
1.25-inch sleeve for square holder (each) P75-125H
1.5-inch sleeve for square holder (each) P75-150H
25 mm sleeve for square holder (each) P75-25H
30 mm sleeve for square holder (each) P75-30H
40 mm sleeve for square holder (each) P75-40H

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL
Request a salesperson call

Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog

Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher

Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes
Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis

Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes
Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:



Copyright 2006-2019
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+