CASTABLE Vacuum Mounting

Vacuum mounting of castable mounting resins significantly improves penetration of voids and provides better edge retention. The LSSA-011 vacuum impregnation unit (Part No. LSSA-011) allows for pouring the resin under maximum vacuum and for mounting multiple specimens.

Metallographic compression mounting presses Vacuum mounting chamber Click here to get a quote
Feature Specification
Bell jar Tilting, retractable pouring arm
Mount size 1 to 2-inch diameter (25-50 mm)
Vacuum Vacuum pump (sold separately)
Dimensions
(W x D x H)
12 x 12 x 12-inch
(300x 300 x 300 mm)
Weight 2.2 lbs (1 kg)

Vacuum Pumps

Description 110V Vacuum Pump 220V Vacuum Pump
Flow Rate 2.5 CFM 7.2 m3/h
Ultimate Vacuum 10 Pa 0.2 Pa
Power 120 W -0.17 hp 370 W - 0.5 hp
Inlet Port ¼” SAE and ½” ACME ports 7/16-inch - 20
Dimensions (W x D x H) 11 x 4.75 x 9-inch
(279 x 120 x 229 mm)
13 x 5.5 x 10-inch
(337 x 138 x 254 mm)
Weight 16.5 lbs (7.5 kg) 22 lbs (10 kg)
Part No. VAC-110 VAC-220
Click here to get a quote

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL
Request a salesperson call

Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog

Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher

Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes
Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis

Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes
Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:



Copyright 2006-2019
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+