Description:

Ceramics in general are relatively brittle with a wide range of thermal and hardness characteristics.

Preparation Challenge:

Proper specimen preparation requires that grinding damage be minimized as early as possible followed by polishing with CMP (chemical mechanical polishing) polishing techniques.

Examples:

Alumina or Sapphire
Metallographic microstructure of alumina

  ALONMetallographic microstructure of ALON or alumina / aluminum nitride

MulliteMetallographic microstructure of Mullite

  Steatite
Metallographic microstructure of Steatite

Beryllium Oxide
Metallographic microstructure of berillium oxide

   

Return to top

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL
Request a salesperson call


Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog



Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher



Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes

Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis



Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes

Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:

Return to top


About Us | Site Map | Web Disclaimer | Terms and Conditions | Contact Us

Copyright 2006-2018
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1 520-882-6598 FAX +1 520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+ PACE Technologies Google+