CLASS 11 - VERY HARD BRITTLE MATERIALS, CERMETS (Tungsten Carbide)
Examples include cermets such as tungsten carbide, glass and minerals.
Description:
CERMET’s are wear resistant, tough materials.
Preparation Challenge: