PACE Technologies Home Page

Metallographic Preparation Procedures - Stainless Steel

| Home | Product Info | MSDS | Procedures | Equipment | Etchants | Contact us |

Metallographic Procedures

Stainless Steel

Description:
Stainless steels have high concentrations of chromium (>12%) and are generally relatively soft compared to heat treated steels. This makes stainless steel more susceptible to smearing.

Preparation Challenge:
Microstructural preparation of stainless steels is very similar to the preparation procedures for iron and steel. The primary difference is that final polishing with nanometer alpha alumina is required to maintain the inclusions in the stainless steel.

Metallographic micrograph for 400 series stainless steel
Metallographic micrograph for stainless steel weld to copper
About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2011
PACE Technologies - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.