The purpose of the grinding step is to remove damage from cutting, planarize the specimen(s), and to remove material approaching the area of interest. It is important to note that it is possible to create more damage in grinding than in sectioning. In other words, it is better to cut as close as possible to the area of interest using the correct abrasive or wafering blade.

Metallographic Abrasive Machining

The following are the most common metallographic abrasives:

Silicon Carbide - SiC is a manufactured abrasive produced by a high temperature reaction between silica and carbon. It has a hexagonal-rhombohedral crystal structure and has a hardness of approximately 2500 HV. It is an ideal abrasive for cutting and grinding because of its hardness and sharp edges. It is also somewhat brittle, and therefore it cleaves easily to produce sharp new edges (self sharpening). SiC is an excellent abrasive for maximizing cutting rates while minimizing surface and subsurface damage. For metallographic preparation, SiC abrasives are used in abrasive blades and for coated abrasive grinding papers ranging from very coarse 60 grit to very fine 1200 grit sizes.

Bonded or coated abrasive papers of SiC are designed so that the abrasive will have a large number of cutting points (negative abrasive rank angle). This is achieved by aligning the abrasive particles approximately normal to the backing. Note that coated abrasives are not quite coplanar, thus SiC papers produce the maximum efficiency (cut rate, stock removal and minimal damage) because new abrasive is exposed as the old abrasive breaks down.




SEM micrograph of 600 grit SiC Abrasive Paper (original mag. 150x)

Alumina - Alumina is a naturally occurring material (Bauxite). It exits in either the softer gamma (mohs 8) or harder alpha (mohs 9, 2000 HV) phase. Alumina abrasives are used primarily as a final polishing abrasive because of its high hardness, and durability; and unlike SiC, alumina breaks down relatively easily to submicron or colloidal particles (Fine Abrasives).

Note that larger coated or bonded grit sizes of alumina are commercially available, however they are not ideal for metallographic applications because they become dull, resulting in lower cut rates and higher surface and subsurface damage.

Diamond - Is the hardest material known to man (mohs 10, 8000 HV). It has a cubic crystal structure, and is available as a natural or an artificial product. Although diamond would be ideal for coarse grinding, its price makes it a very inefficient grinding material for anything except for hard ceramics. For metallographic applications, polycrystalline diamond is recommended as a rough polishing abrasive (PC diamond).

Grinding Parameters

Successful grinding is also a function of the following parameters:

  1. Grinding Pressure
  2. Relative Velocities
  3. Grinding Direction



ABRASIVE GRINDING SELECTION GUIDELINES CHART

Material

Objective

Recommendation

Soft non-ferrous metals (aluminum, copper, brass, tin, zinc, lead, etc.)

Minimize deformation on the surface

320 grit SiC paper
400 grit SiC paper
600 grit SiC paper
800 grit SiC paper
1200 grit SiC paper

Soft ferrous metals (low carbon steels, stainless steel, case hardened steel, etc.)

Minimize deformation and secondary phase damage

240 grit SiC paper
320 grit SiC paper
400 grit SiC paper
600 grit SiC paper
800 grit SiC paper
1200 grit SiC paper

Hard ferrous metals (high carbon steel, tool steel, case hardened steel, etc.)

Planarize specimen and minimize specimen deformation

180 grit SiC paper
240 grit SiC paper
320 grit SiC paper
400 grit SiC paper
600 grit SiC paper

Super alloys (high nickel and cobalt alloys, titanium alloys)

Minimize deformation

240 grit SiC paper
320 grit SiC paper
400 grit SiC paper
600 grit SiC paper

Ceramics, ceramic matrix composites, and minerals

Minimize surface and subsurface damage (fracturing and chipping)

30 um polycrystalline diamond on a Metal Mesh cloth

Metal matrix composites, polymer matrix composites

Minimize composite fracturing and minimizing matrix deformation

240 or 320 grit SiC paper

  • Soft non-ferrous metals - Initial grinding is recommended with 320 grit SiC abrasive paper followed by 400, 600, 800 and 1200 grit SiC paper. Because these materials are relatively soft they do not easily break down the SiC paper. Thus initial grinding with 320 grit is generally sufficient for minimizing initial deformation and yet maintain adequate removal rates. For extremely soft materials such as tin, lead and zinc it is also recommended that the abrasive paper be lightly coated with a paraffin wax. The wax reduces the tendency of the SiC abrasive to embed into the soft specimen.
  • Soft ferrous metals - are relatvely easy to grind with the depth of deformation being a major consideration. 240 grit SiC abrasives provide a good initial start with subsequent use of 320, 400, 600, 800 and 1200 grit SiC.
  • Hard ferrous metals - require more aggressive abrasives to achieve adequate material removal. Thus coarse SiC abrasives (120 or 180 grit) are recommended for stock removal requirements. Once planarity and the area of interest are obtained a standard 240, 320, 400 and 600 grit series is recommended.
  • Super alloys - are generally of moderate hardness but have extremely stable elevated temperature characteristics and corrosion resistance. The procedures for preparing super alloys is very similar to that for most non-ferrous metals.
  • Ceramics - are extremely hard, corrosion resistant and brittle materials. They fracture producing both surface and subsurface damage. Proper grinding minimizes both of these forms of damage. This requires the application of a semi-fixed abrasive which are held rigidly for grinding but can be dislodged under high stress in order to minimize subsurface damage. The use of a metal mesh cloth (CERMESH cloth) with an applied abrasive accomplishes both of these goals. The abrasive size is also important because very coarse abrasives will remove material quickly but can seriously damage the specimen. For ceramics, consideration of the damage produced at each preparation step is critical to minimizing the overall preparation sequence.
  • Composites - are perhaps the most difficult specimens to prepare because of the wide range of properties for the materials used. For example, a metal matrix composite (MMC) such as silicon carbide ceramic particles in an aluminum metal matrix is a difficult specimen to prepare. This composite contains extremely hard/brittle ceramic particles dispersed in a relatively soft/ductile metal matrix. As a rule of thumb, initial grinding should focus on metal planarization and grinding to the area of interest. The secondary grinding steps require focusing on the ceramic particles and typically requires the use of diamond abrasives.
Return to top


ABRASIVE GRINDING PROCESS DESCRIPTION

The machine parameters which affect the preparation of metallographic specimens include: grinding/polishing pressure, relative velocity distribution, and the direction of grinding/polishing.

Grinding Pressure

Grinding/polishing pressure is dependent upon the applied force (pounds or Newtons) and the area of the specimen and mounting material. Pressure is defined as the Force/Area (psi, N/m2 or Pa). For specimens significantly harder than the mounting compound, pressure is better defined as the force divided by the specimen surface area. Thus, for larger hard specimens higher grinding/polishing pressures increase stock removal rates, however higher pressure also increases the amount of surface and subsurface damage. Note for SiC grinding papers, as the abrasive grains dull and cut rates decrease, increasing grinding pressures can extend the life of the SiC paper.

Higher grinding/polishing pressures can also generate additional frictional heat which may actually be beneficial for the chemical mechanical polishing (CMP) of ceramics, minerals and composites. Likewise for extremely friable specimens such as nodular cast iron, higher pressures and lower relative velocity distributions can aid in retaining inclusions and secondary phases.

Relative Velocity

Current grinding/polishing machines are designed with the specimens mounted in a disk holder and machined on a disk platen surface. This disk on disk rotation allows for a variable velocity distribution depending upon the head speed relative to the base speed.

Head Speed (rpm)

Base Speed (rpm)

Relative Velocity Distribution

Characteristic

Application

150

300 to 600

High

  • Aggressive stock removal
  • Differential grinding across the specimen surface
  • Useful for gross removal on hard specimens
  • 150

    150

    Minimal

  • Matching head and base speed in the same direction eliminates relative velocity distributions
  • Uniform stock removal
  • Low stock removal
  • Produces minimal damage
  • Provides superior flatness over the specimen
  • Useful for retaining inclusions and brittle phases
  • For high stock removal, a slower head speed relative to a higher base speed produces the most aggressive grinding/ polishing operation. The drawback to high velocity distributions is that the abrasive (especially SiC papers) may not breakdown uniformly, this can result in non-uniform removal across the specimen surface. Another disadvantage is that the high velocity distributions can create substantially more specimen damage, especially in brittle phases. In all cases, it is not recommended to have the head rotating contra direction to the base because of the non-uniform removal and abrasive break-down which occurs.

    Minimal relative velocity distributions can be obtained by rotating the head specimen disk at the same rpm and same direction as the base platen. This condition is best for retaining inclusions and brittle phases as well as for obtaining a uniform finish across the entire specimen. The disadvantage to low relative velocity distributions is that stock removal rates can be quite low.

    In practice, a combination of a high velocity distribution (150 rpm head speed/ 300 - 600 rpm base speed) for the initial planarization or stock removal step, followed by a moderate speed and low velocity distribution (120-150 rpm head speed/ 150 rpm base speed) step is recommended for producing relatively flat specimens. For final polishing under chemical mechanical polishing (CMP) conditions where frictional heat can enhance the chemical process, high speeds and high relative velocity distributions can be useful as long as brittle phases are not present (e.g. monolithic ceramics such as silicon nitride and alumina).

    Grinding Direction

    The orientation of the specimen can have a significant impact on the preparation results, especially for specimens with coatings. In general, when grinding and polishing materials with coatings the brittle component should be kept in compression. In other words, for brittle coatings the direction of the abrasive should be through the coating and into the substrate. Conversely, for brittle substrates with ductile coatings, the direction of the abrasive should be through the brittle substrate into the ductile coating.


    Return to top


    ABRASIVE GRINDING RECOMMENDED PROCEDURES Application (Fixed-abrasive Grinding)
    • Start with the finest abrasive possible (typically 240 or 320 grit abrasive paper) Note: Only use coarser grit for very heavy stock removal
    • Apply lubricant to abrasive surface
      • Most commonly water
      • Water soluble oils for water sensitive specimens
    • Rinse specimens thoroughly before proceeding to the next finer abrasive
    Application (CERMESH metal mesh cloth)
    1. Apply CERMESH metal mesh cloth to flat base surface (Suggestion - peel back protective paper at one corner and align and place on base surface. Pull protective paper with one hand while guiding metal mesh cloth with other hand)
    2. Pre-charge CERMESH metal mesh cloth with DIAMAT polycrystalline diamond
    3. To avoid tearing the cloth, begin initial grinding at 50% force to set specimen(s) to metal mesh cloth
    4. Ramp-up force gradually
    5. Add abrasive as required
    6. Rinse CERMESH metal mesh cloth with water at the end of the grinding cycle to remove swarf debris
    Return to top


    ABRASIVE GRINDING TROUBLE SHOOTING

    Symptom

    Cause

    Action

    Uneven grinding across the specimen and mount

  • Improper tracking of specimen over abrasive paper
  • Orient specimen in holder so that the hardest portion of the specimen/mount tracks over the entire abrasive paper (uniform degradation of paper)
  • Excessive vibration in machine

  • Too high a load or too low a speed
  • Inadequate machine design
  • Improper lubricant
  • Reduce initial grinding force or increase grinding speed
  • Check with equipment vendor for equipment upgrades
  • Increase lubricant flow and/or use a water-soluble lubricant
  • Embedding of fractured abrasive grains

  • Common in the grinding of very soft materials
  • Apply a thin coat of wax on the abrasive surface prior to grinding

  • Return to top



    SiC ABRASIVE PAPER (w/PSA) SiC ABRASIVE PAPER

    8-inch ABRASIVE PAPER (PSA)

    Description

    Diameter (inches)

    Units/pkg

    Catalog Number

    60 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-060P8-100

    120 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-120P8-100

    180 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-180P8-100

    240 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-240P8-100

    320 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-320P8-100

    360 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-360P8-100

    400 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-400P8-100

    600 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-600P8-100

    800 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-800P8-100

    1000 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-1000P8-100

    1200 grit SiC paper w/ PSA adhesive

    8

    100

    SIC-1200P8-100

    10-inch ABRASIVE PAPER (PSA)

    Description

    Diameter (inches)

    Units/pkg

    Catalog Number

    60 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-060P10-100

    120 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-120P10-100

    180 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-180P10-100

    240 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-240P10-100

    320 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-320P10-100

    400 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-400P10-100

    600 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-600P10-100

    800 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-800P10-100

    1200 grit SiC paper w/ PSA adhesive

    10

    100

    SIC-1200P10-100

    12-inch ABRASIVE PAPER (PSA)

    Description

    Diameter (inches)

    Units/pkg

    Catalog Number

    60 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-060P12-100

    120 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-120P12-100

    180 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-180P12-100

    240 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-240P12-100

    320 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-320P12-100

    360 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-360P12-100

    400 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-400P12-100

    600 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-600P12-100

    800 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-800P12-100

    1000 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-1000P12-100

    1200 grit SiC paper w/ PSA adhesive

    12

    100

    SIC-1200P12-100


    SiC ABRASIVE PAPER (Plain backed)

    8-inch ABRASIVE PAPER (Plain Backed)

    Description

    Diameter (inches)

    Units/pkg

    Catalog Number

    60 grit SiC paper plain backed

    8

    100

    SIC-2108-060

    120 grit SiC paper plain backed

    8

    100

    SIC-2108-120

    180 grit SiC paper plain backed

    8

    100

    SIC-2108-180

    240 grit SiC paper plain backed

    8

    100

    SIC-2108-240

    320 grit SiC paper plain backed

    8

    100

    SIC-2108-320

    360 grit SiC paper plain backed

    8

    100

    SIC-2108-360

    400 grit SiC paper plain backed

    8

    100

    SIC-2108-400

    600 grit SiC paper plain backed

    8

    100

    SIC-2108-600

    800 grit SiC paper plain backed

    8

    100

    SIC-2108-800

    1000 grit SiC paper plain backed

    8

    100

    SIC-2108-1000

    1200 grit SiC paper plain backed

    8

    100

    SIC-2108-1200

    12-inch ABRASIVE PAPER (Plain Backed)

    Description

    Diameter (inches)

    Units/pkg

    Catalog Number

    60 grit SiC paper plain backed

    12

    100

    SIC-2112-060

    120 grit SiC paper plain backed

    12

    100

    SIC-2112-120

    180 grit SiC paper plain backed

    12

    100

    SIC-2112-180

    240 grit SiC paper plain backed

    12

    100

    SIC-2112-240

    320 grit SiC paper plain backed

    12

    100

    SIC-2112-320

    360 grit SiC paper plain backed

    12

    100

    SIC-2112-360

    400 grit SiC paper plain backed

    12

    100

    SIC-2112-400

    600 grit SiC paper plain backed

    12

    100

    SIC-2112-600

    800 grit SiC paper plain backed

    12

    100

    SIC-2112-800

    1000 grit SiC paper plain backed

    12

    100

    SIC-2112-1000

    1200 grit SiC paper plain backed

    12

    100

    SIC-2112-1200

    DOUBLE SIDED ADHESIVE (for non PSA paper)

    Description

    Diameter (inches)

    Quantity

    Catalog Number

    Double Sided Adhesive

    8

    10/pkg.

    DSA-08

    Double Sided Adhesive

    10

    10/pkg.

    DSA-10

    Double Sided Adhesive

    12

    10/pkg.

    DSA-12


    Return to top

    ZIRCONIA ABRASIVES PAPER

    ZIRCONIA COURSE GRINDING DISKS

    Description

    Units/pkg

    Catalog Number

    8-inch 60 grit Zirconia paper (PSA)

    25/box

    ZR-060P08-25

    12-inch 60 grit Zirconia paper (PSA)

    25/box

    ZR-060P12-25


    Return to top


    ABRASIVE ROLLS and BELTS

    ABRASIVE BELTS (4" x 36")

    Description

    Units/pkg

    Catalog Number

    60 grit Zirconia belt

    5/box

    ZrO2-B060

    120 grit Zirconia belt

    5/box

    ZrO2-B120

    60 grit SiC belt

    10/box

    SIC-B60

    80 grit SiC belt

    10/box

    SIC-B80

    120 grit SiC belt

    10/box

    SIC-B120

    180 grit SiC belt

    10/box

    SIC-B180

    240 grit SiC belt

    10/box

    SIC-B240

    320 grit SiC belt

    10/box

    SIC-B320

    400 grit SiC belt

    10/box

    SIC-B400

    ABRASIVE ROLLS (3-7/16" width, 60-feet length, 5/8" core)

    Description

    Units/pkg

    Catalog Number

    240 grit SiC roll

    each

    SIC-240R-60

    320 grit SiC roll

    each

    SIC-320R-60

    400 grit SiC roll

    each

    SIC-400R-60

    600 grit SiC roll

    each

    SIC-600R-60


    Return to top
    About Us | Site Map | Disclaimer and Legal Information | Contact Us

    Copyright © 2006
    Pace Technologies, Inc. - 1802 W. Grant Rd. No. 102 - Tucson, AZ 85745 USA
    Telephone 520-882-6598 FAX 520-882-6599.
    All Rights Reserved.