Equipment - Metallographic Polishers

Metallographic Laboratory Automated Polishers

Metallographic Automated Power Polishing Heads

Home ] Mechanical ] Individual ] Central ] Individual/Central ] Equipment Listing ] Consumables ] Quote Request ]




Quick Selection Guide
Automated Grinding/ Polishing Machines

Description

Speed (rpm)

Base Polisher

Catalog Number

GRIPOMAT

Adjustable

GRIPO series

30-08

FORCIMAT

120 rpm

GRIPO series

30-09

DIGIMAT

150 rpm

DIGISET series

45-01

DIGIMAT+

150 rpm

DIGISET series

45-02

Return to top


Mechanical Automated Grinder/Polishers

Feature

Description

Application of Force

Individual

Head speed

Variable

Force

2.25 lbs to 10 lbs

Compatibility

GRIPO series polishers

Accessories for GRIPOMAT Automated Polishing Heads

Specimen Holder

Part Number

Specimen holder for GRIPOMAT (3 specimen rings)

32-03

1-in diameter rings

33-03

1.25-in diameter rings

33-05

1.5-in diameter rings

33-04


Return to top


Individual FORCIMAT Automated Grinder/Polishers

 

Feature

Description

Application of Force

Individual

Head speed

120 rpm, contra or complimentary

Samples

1-4

Force

1.1 lbs to 13.5 lbs
(5N to 60N)

Compatibility

GRIPO series polishers

Controls

Microprocessor with touch pad

Construction

GRP (glass reinforced plastic)

Voltage

110V, 60 Hz

Dimensions (WxHxL)

8.7" x 18" x 15"

Weight

35 lbs









Metallographic Forcimet Polishing Head
 

Accessories for FORCIMAT Automated Polishing Heads

Specimen Holder

Part Number

Specimen holder for FORCIMAT (4 specimen rings)

33-01

1-in diameter rings

33-03

1.25-in diameter rings

33-05

1.5-in diameter rings

33-04

Blank holder

33-06

2-in diameter specimen holder

33-07


Return to top


Central DIGIMAT Automated Grinder/Polishers

 

Feature

Description

Application of Force

Central

Head speed

150 rpm, contra or complimentary

Samples

3-10 (dependent upon diameter of and polisher size)

Force

11.25 lbs to 81 lbs
(50N to 360N)

Compatibility

DIGISET series polishers

Controls

Microprocessor with touch pad

Construction

GRP (glass reinforced plastic)

Voltage

110V, 60 Hz

Dimensions (WxHxL)

9" x 18" x 15"

Weight

64 lbs






 

Accessories for DIGIMAT Automated Polishing Heads

Central specimen holder for 8-inch polishers (5.1-inch outside diameter of holder)

Description

Part Number

1-in diameter holder for 3 to 6 specimens

45-14

1.25-in diameter holder for 3 to 6 specimens

45-15

1.5-in diameter holder for 3 to 6 specimens

45-16

5.1-inch diameter specimen loading plate

45-10

Central specimen holder for 12-inch polishers (6.7-inch outside diameter of holder)

Description

Part Number

1-in diameter holder for 3 to 10 specimens

45-35

1.25-in diameter holder for 3 to 8 specimens

45-36

1.5-in diameter holder for 3 to 6 specimens

45-37

6.7-inch diameter specimen loading plate

45-30

Return to top


Individual / Central DIGIMAT+ Automated Grinder/Polishers

 

Feature

Description

Application of Force

Individual / Central

Head speed

150 rpm, contra or complimentary

Samples

Central 3-10 samples
Individual 1-6 samples

Force

Central 11.25 to 81 lbs
Individual 1.1 to 13.5 lbs

Compatibility

DIGISET series polishers

Controls

Microprocessor with touch pad

Construction

GRP (glass reinforced plastic)

Voltage

110V, 60 Hz

Dimensions (WxHxL)

9" x 18" x 15"

Weight

53 lbs



Metallographic Digimat-plus polishing head
 

Accessories for DIGIMAT+ Automated Polishing Heads

Central specimen holder for 8-inch polishers (5.1-inch outside diameter of holder)

Description

Part Number

1-in diameter holder for 3 to 6 specimens

45-14

1.25-in diameter holder for 3 to 6 specimens

45-15

1.5-in diameter holder for 3 to 6 specimens

45-16

5.1-inch diameter specimen loading plate

45-10

Central specimen holder for 12-inch polishers (6.7-inch outside diameter of holder)

Description

Part Number

1-in diameter holder for 3 to 10 specimens

45-35

1.25-in diameter holder for 3 to 8 specimens

45-36

1.5-in diameter holder for 3 to 6 specimens

45-37

6.7-inch diameter specimen loading plate

45-30

Individual Specimen holders for DIGIMAT+ Automated Polishing Heads

Specimen Holder

Part Number

1-in diameter, 6 specimens

45-54

1.25-in diameter, 6 specimens

45-55

1.5-in diameter, 4 specimens

45-56

2-in diameter, 3 specimens

45-58

Blank holder

33-06


Return to top

About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2006
Pace Technologies, Inc. - 1802 W. Grant Rd. No. 102 - Tucson, AZ 85745 USA
Telephone 520-882-6598 FAX 520-882-6599.
All Rights Reserved.