Metallographic Composite Disks Grinding

Metallographic Composite disks

Composite Disks

Application Guideline ] Trouble Shooting ] Product Description ] [ Home ]


Composite grinding disks are an alternative to intermediate grinding and polishing. PACE Technologies composite disk vary slightly from other competitive products in that they are precharged with diamond. This allows the disks to cut faster and longer. Two disks types are available, the ORION composite polishing disk is precharged with 3 micron diamond, whereas the SIRIUS composite disk is precharged with 9 micron diamond.

The SIRIUS composites grinding disks offer an alternative to grinding with 320-600 grit SiC papers, and the ORION composite disk offer an excellent alternative to rough polishing with 3-6 micron diamond.

Close-up of Composite Grinding Disk

Return to top


APPLICATION GUIDELINES (Composite Disks)

  • Apply magnetic backed composite disk to reciever wheel
  • Apply diamond suspension as required
  • Rinse with water to clean plate


Return to top



TROUBLE SHOOTING GUIDELINES (Composite Disks)

Symptom

Cause

Action

Uneven grinding/polishing

Surface wearing out of flat

Replace disk and grind/polish with the head speed matching the base speed and running in the complementary direction

Large scratches or gouges in sample

Contaminated disk

Replace and use correct diamond suspension size


Return to top



COMPOSITE DISK PRODUCT DESCRIPTIONS

Description

Size

Catalog Number

 

ORION Composite Disk precharged with 3 micron diamond (magnetic steel backing)

8-inch
10-inch
12-inch

ORION-MD08
ORION-MD10
ORION-MD12

Composite grinding plates

SIRIUS Composite Disk precharged with 9 micron diamond (magnetic steel backing)

8-inch
10-inch
12-inch

SIRIUS-MD08
SIRIUS-MD10
-MD12

Compressed Non-flammable gas
each
AIR-1000


Return to top

About Us | Site Map | Disclaimer and Legal Information | Contact Us

Copyright © 2011
PACE Technologies - 3601 E. 34th St. - Tucson, AZ 85713 USA
Telephone +1 520-882-6598 FAX +1 520-882-6599.
All Rights Reserved.