Metallographic equipment or metallography sample preparation equipment has been designed to minimize damage or to remove both surface and subsurface damage to the metallographic specimens microstructure. Metallographic abrasive saws are designed to cut at lower speeds so as to minimize microstructural damage. Additionally, metallographic polishing machines must be designed to minimize subsurface and surface damage to the microstructure as opposed to aggressive abrasive grinding used in other industries. Metallograhic equipment results in properly prepared, artifact free surface that can be properly analyzed on metallurgical or metallographic microscopes.