The PICO-155S Precision Wafering Saw combines advanced digital controls with robust design, featuring a 5-inch touchscreen for intuitive operation. It offers a 2-inch cutting capacity and dual nozzle cooling to optimize cutting conditions. With a variable speed range of 200-1500 rpm displayed digitally, it provides flexibility for various materials. The micrometer feed accuracy of 2 microns ensures precision, making the PICO-155S ideal for labs focused on accuracy and efficiency in sectioning.
| Parameter | Specification |
|---|---|
| Control | 5-inch Touchscreen with Digital LED Display |
| Cutting Capacity | Max. diameter 50 mm (2 inches) |
| Coolant System | Dual nozzle with pump |
| Table Feed | 75 mm to 175 mm (3 to 7 inches) |
| Arbor Size | 12.7 mm (0.5 inches) |
| Variable Speed (RPM) | 200-1500 rpm continuously adjustable with digital speed display |
| Cutting Load | 0-1500 gram load |
| Micrometer Feed Distance | 0 to 25 mm (0 to 1 inch) |
| Micrometer Accuracy | 2 microns |
| Electrical Specification | 110V/220V (50/60 Hz) single phase |
| Motor Power | 125W (24V) |
| Dimensions (WxDxH) - Hood Closed | 480 x 580 x 370 mm (19 x 23 x 14 inches) |
| Dimensions (WxDxH) - Hood Open | 480 x 740 x 480 mm (19 x 29 x 19 inches) |
| Weight | 30 kg (66 lbs) |
| Catalog Number | PICO-155S |