GIGA-S Vibratory Polisher
GIGA-S Metallographic Vibratory Polisher
Item ID: GIGA-S
A PZT-driven vibratory polisher with interchangeable 9-inch and 12-inch bowls for low-relief finishes. Ideal for EBSD sample preparation with pulse mode for stain-free results.
Features
- PZT motor for precise, consistent vibration control
- Interchangeable 9-inch and 12-inch polishing bowls
- Pulse mode prevents staining on finished samples
- Leak-free two-part bowl for mess-free operation
Technical Specifications
| Parameter | Specification |
|---|---|
| Polishing Bowl Size | 9-inch or 12-inch interchangeable bowls |
| Drive Mechanism | PZT Motor (Piezoelectric Vibration) |
| Frequency | 0-220 Hz |
| Electrical Specification | 110 / 240V (50/60 Hz) |
| Construction | Aluminum casting with SMC injection-molded cover |
| Dimensions (WxDxH) | 16 x 20 x 16 inches (420 x 500 x 410 mm) with hood closed |
| Weight | 135 lbs (62 kg) |
| Part Number | GIGA-S |