The TeraVAC and TeraVAC Pro vacuum impregnation systems are designed to improve resin penetration in samples with voids and porosity. The TeraVAC offers a simple, economical solution with vacuum pouring, room-pressure curing, and a tilting, retractable pouring arm for ease of use and reliable results. The TeraVAC Pro builds on this capability with programmable, automated control of vacuum and cycle parameters, a larger chamber capacity, an integrated rotating table for efficient mold positioning, and a user-friendly, low-noise design suited for higher-throughput laboratory environments.
| Parameter | Specification |
|---|---|
| Bell Jar | Tilting, retractable pouring arm |
| Mount Sizes | 1, 1.25, 1.5, and 2-inch (25, 30, 40, and 50 mm) |
| Vacuum | Vacuum pump (sold separately) |
| Dimensions (WxDxH) | 12 x 12 x 12 inches (300 x 300 x 300 mm) |
| Weight | 2.2 lbs (1 kg) |
| Catalog Number | TeraVAC |
| Parameter | Specification |
|---|---|
| Control Interface | 5-inch touch screen |
| Chamber Capacity | Up to 12 samples - 1.5-inch (40 mm) diameter |
| Vacuum Range | 0-90 kPa |
| Dimensions (WxDxH) | Open: 20 x 18 x 25-inch (507 x 464 x 300 mm) / Closed: 20 x 18 x 10.5-inch (507 x 646 x 267 mm) |
| Weight | 40 lbs (18 kg) |
| Catalog Number | TeraVAC Pro |