ATTO-1000S Controlled Removal Polisher
The ATTO-1000S Controlled Removal Polisher is engineered for precise material removal and surface preparation in metallographic sample preparation. This advanced machine offers both precision-controlled removal and metered removal capabilities, making it ideal for applications that demand high accuracy. With its robust construction and intuitive controls, the ATTO-1000S ensures consistent and reliable performance, making it an essential tool for laboratories focused on achieving meticulous sample preparation results.
ATTO-1000S Controlled Removal Polisher
ATTO-1000S - Precision Controlled Removal Polisher
Features
- Controlled Micro-Precision Removal: Ensures precise material removal with high accuracy for delicate samples.
- Versatile Polishing Capabilities: Suitable for IC Flip Chips, SEM, FIB, TEM, AFM, EBSD, petrographic, and optical analysis.
- Advanced Control Panel: Features a 7-inch touchscreen panel with micrometer adjustable pitch and roll control for exacting results.
- Robust Design: Constructed with durable materials for reliable performance in demanding environments.
Technical Specifications - ATTO-1000S
| Parameter | Specification |
|---|---|
| Polishing Control | Micrometer adjustable pitch and roll control |
| Wheel Speed | 0-350 rpm |
| Head Speed | 0-150 rpm (in 1 rpm increments) |
| Sample Load | 0-300 grams |
| Drive Mechanism | Servo Motor with Torque Control |
| LCD Display | Real-time removal with 0.2 micron resolution |
| Dimensions (WxDxH) | 27.6 x 16.9 x 22.8 inches (700 x 430 x 580 mm) |
| Weight | 125.7 lbs (57 kg) |
| Part Number | ATTO-1000S |