Proper cleaning is essential to ensure contamination-free metallographic specimens and accurate microstructural analysis. PACE Technologies offers specialized cleaning consumables, including ultrasonic solutions and alcohol rinses, designed to effectively remove abrasive residues, polishing slurries, and embedded particulates. Whether for intermediate or final cleaning, our products help preserve surface integrity and prevent corrosion, supporting reliable and repeatable results.
View in our shop:
Cleaning and drying are critical but often underestimated steps in metallographic specimen preparation. Proper cleaning removes abrasive residues and particulate contamination that could distort analysis results. The process includes intermediate cleaning to prevent cross-contamination between steps and final cleaning to eliminate polishing compounds before examination. When executed correctly, these steps improve accuracy, reduce artifacts, and protect specimen surfaces from corrosion and staining.
Effective cleaning and drying procedures are essential for preventing contamination, preserving surface quality, and ensuring accurate metallographic analysis. This section outlines the recommended practices for both intermediate and final cleaning, as well as drying techniques and corrosion protection.
Intermediate cleaning prevents abrasive cross-contamination between polishing steps. Begin by rinsing the specimen and holder with water, using a cotton swab to remove loose abrasive and swarf. For deeper cleaning, use an ultrasonic cleaner with a suitable surfactant to eliminate embedded contaminants in specimen pores, mounting cavities, or holder crevices. Finish with a tap water rinse. While air drying is optional at this stage, it is recommended to avoid moisture retention.
Final cleaning should occur immediately after polishing to prevent the crystallization or agglomeration of fine abrasives like colloidal silica or NANOMETER alumina. Rinse the polishing pad and specimen with distilled or deionized water for the last 10–15 seconds of polishing to clean both surfaces. For challenging residues, gently scrub the specimen with a cotton swab dipped in alcohol. This same cleaning method is also recommended after etching to ensure a clean surface for microscopic analysis.
After cleaning, specimens should be placed in an ultrasonic bath followed by a rinse or dip in alcohol. Alcohol displaces water, promoting faster and more complete drying. Use compressed air or a heated oven to dry the specimen surface thoroughly. To prevent corrosion or staining—especially in porous mounts—dip the specimen in an organic corrosion inhibitor. This forms a protective coating and minimizes oxidation during storage.
Residues, stains, and drying inconsistencies can compromise the accuracy of metallographic analysis. The table below outlines common cleaning and drying issues, their likely causes, and corrective actions to restore specimen integrity.
| Symptom | Cause | Action |
|---|---|---|
| Specimen surface has a thin "matte like" film | Thin coating of NANOMETER alumina particles | Lightly remove particles with a cotton swab and alcohol |
| Specimen surface has a crystallized residue | Crystallized colloidal silica | Repolish and rinse polishing pad and specimen with water during the last 10–15 seconds of polishing |
| Water spots on specimen | Hard water rinsing | Lightly repolish, rinse with deionized water, follow with alcohol rinse, and dry with compressed air |
| Pits in specimen after rinsing | Corrosion of water-soluble phases | Clean with organic solvents such as alcohol to prevent corrosion |
| Inability to completely dry specimen | Water retained in cracks or pores | Dip specimen in an alcohol-based corrosion inhibitor to promote evaporation and form a protective coating |
PACE Technologies offers a comprehensive selection of cleaning and drying consumables designed to support intermediate and final cleaning, specimen preservation, and corrosion protection. Below is a summary of available products, quantities, catalog numbers, and corresponding images where applicable.
| Description | Quantity | Catalog Number |
|---|---|---|
| Organic Corrosion Inhibitor (100X concentrate in IPA) | 32 oz (0.97 L) | PCC-7500-32 |
| Urethane Spray Coating | Each | URE-1000 |
| 1.25-inch Plastic Storage Container | 25/pkg | STORE-0125 |