Rockwell Hardness Testers
Rockwell Hardness Testers by PACE Technologies provide dependable and accurate hardness measurement solutions tailored for various metallographic applications. Designed for modern material testing, they deliver precise results across various Rockwell scales, ensuring consistent performance and compliance with industry standards.
Rockwell
Superficial & Dual Rockwell / Superficial
OMEGA-RT Manual Rockwell Hardness Tester
OMEGA-RT - Manual Rockwell Hardness Tester
Features
- Rockwell Scales: HRA, HRB, HRC
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Manual Loading Control: Provides operator control for precise testing.
Technical Specifications - OMEGA-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 7.2 x 21.5 x 29.7 inches (182 x 546 x 755 mm) |
| Weight | 200 lbs (90 kg) |
| Part Number | OMEGA-RT |
OMEGA-RT2 Manual Rockwell Hardness Tester
OMEGA-RT2 - Manual Rockwell Hardness Tester
Features
- Rockwell Scales: HRA, HRB, HRC
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Manual Loading Control: Provides operator control for precise testing.
Technical Specifications - OMEGA-RT2
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 9.6 x 20.5 x 27.6-inch (245 x 520 x 700mm) |
| Weight | 172 lbs (78 kg) |
| Part Number | OMEGA-RT2 |
OMEGA-DIGI-RT Digital Rockwell Hardness Tester
OMEGA-DIGI-RT - Digital Rockwell Hardness Tester
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Digital Interface: Provides easy operation and precise control with auto hardness conversion.
Technical Specifications - OMEGA-DIGI-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 1-60 seconds |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 7 x 21.5 x 30 inches (182 x 546 x 755 mm) |
| Weight | 198 lbs (90 kg) |
| Part Number | OMEGA-DIGI-RT |
OMEGA-RT-60/150 Digital Rockwell Hardness Tester
OMEGA-RT-60/150 - Digital Rockwell Hardness Tester
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Adjustable Dwell Time: Ensures consistent and accurate testing.
Technical Specifications - OMEGA-RT-60/150
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 1-60 seconds |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 8.5 x 20 x 28 inches (215 x 520 x 700 mm) |
| Weight | 172 lbs (78 kg) |
| Part Number | OMEGA-RT-60/150 |
OMEGA-AUTO-RT Automated Rockwell Hardness Tester
OMEGA-AUTO-RT - Automated Rockwell Hardness Tester
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Fully Automated Operation: Ensures consistent and repeatable results with minimal operator intervention.
Technical Specifications - OMEGA-AUTO-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 1-60 seconds |
| Instrument Throat Height | 11 inches (280 mm) |
| Dimensions (WxDxH) | 9 x 24 x 34.8 inches (225 x 615 x 885 mm) |
| Weight | 275 lbs (125 kg) |
| Part Number | OMEGA-AUTO-RT |
OMEGA-RST-15/150 Digital Dual Rockwell / Superficial Hardness Tester
OMEGA-RST-15/150 - Digital Dual Rockwell / Superficial Hardness Tester
Features
- Versatile Testing: Capable of both Rockwell and Superficial Rockwell hardness testing.
- Adjustable Test Forces: Offers a wide range of test forces for different materials and applications.
- Digital Precision: Includes digital controls for accurate and repeatable testing results.
Technical Specifications - OMEGA-RST-15/150
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV, HR15N, HR30N, HR45N, HR15T, HR30T, HR45T |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.3 inches (165 mm) |
| Dimensions (WxDxH) | 8.5 x 20 x 28 inches (215 x 520 x 700 mm) |
| Weight | 175 lbs (80 kg) |
| Part Number | OMEGA-RST-15/150 |
OMEGA-DIGI-RST Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester
OMEGA-DIGI-RST - Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester
Features
- Semi-Automated Operation: Combines manual and automated features for efficient testing.
- Digital Precision: Includes digital controls for accurate and repeatable testing results.
- Versatile Testing: Capable of both Rockwell and Superficial Rockwell hardness testing.
Technical Specifications - OMEGA-DIGI-RST
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 8.8 x 24 x 35 inches (225 x 615 x 885 mm) |
| Weight | 265 lbs (120 kg) |
| Part Number | OMEGA-DIGI-RST |
OMEGA-AUTO-RST Automated Dual Rockwell / Superficial Hardness Tester
OMEGA-AUTO-RST - Automated Dual Rockwell / Superficial Hardness Tester
Features
- Fully Automated Testing: Offers complete automation for Rockwell and Superficial Rockwell hardness testing.
- High Throughput: Designed for efficient, high-volume testing environments.
- Precision Control: Provides accurate and consistent results with minimal operator intervention.
Technical Specifications - OMEGA-AUTO-RST
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 9 x 24 x 34.8 inches (225 x 615 x 885 mm) |
| Weight | 275 lbs (125 kg) |
| Part Number | OMEGA-AUTO-RST |