Brinell / MacroVickers Hardness Testers
Brinell and MacroVickers Hardness Testers from PACE Technologies deliver precise, reliable hardness measurements for metallographic applications. Built to meet modern material testing demands, they provide accurate results across various test forces and sample sizes. Whether for routine quality control or advanced research, our testers ensure material integrity and compliance with industry standards.
OMEGA-5000-VZ Semi-Automated MacroVickers Hardness Tester
OMEGA-5000-VZ - Semi-Automated MacroVickers Hardness Tester
Features
- Test Force Range: 1kgf to 50kgf for versatile testing needs.
- Precision Optics: Includes 10X and 20X objectives for clear and detailed observations.
- Automated Shifting: Automatically shifts between objective and indenter for efficient testing.
Technical Specifications - OMEGA-5000-VZ
| Parameter | Specification |
|---|---|
| Test Force Range | 1kgf, 2kgf, 2.5kgf, 3kgf, 5kgf, 10kgf, 20kgf, 30kgf, 50kgf |
| Optical Magnification | 100X, 200X (10X and 20X objectives) |
| Loading Method | Automatic (Loading/Dwell/Unloading) |
| Dwell Time | Adjustable 5-60 seconds |
| Resolution | 0.25µm, 0.125µm |
| Construction | Aluminum and stainless steel |
| Maximum Sample Height | 6.7 inches (170 mm) |
| Dimensions (WxDxH) | 11 x 21 x 25 inches (280 x 530 x 630 mm) |
| Weight | 77 lbs (35 kg) |
| Part Number | OMEGA-5000-VZ |
OMEGA-HB Manual Brinell Hardness Tester
OMEGA-HB - Manual Brinell Hardness Tester
Features
- Wide Test Force Range: 62.5 to 3000 Kgf for robust testing across various materials.
- Optical Measuring Device: Equipped with a 20X optical scope for accurate measurement.
- Sturdy Construction: Designed for long-term durability in demanding environments.
Technical Specifications - OMEGA-HB
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 3000 Kgf |
| Optical Measuring Device | 20X Optical scope |
| Max Height of Specimen | 8.1 inches (205 mm) |
| Throat Height | 5.3 inches (135 mm) |
| Power Requirements | 110V/60 Hz; 220V/50 Hz |
| Dimensions (WxDxH) | 9.3 x 21.5 x 29.7 inches (235 x 545 x 755 mm) |
| Weight | 290 lbs (130 kg) |
| Part Number | OMEGA-HB |
OMEGA-HB-3000 Digital Brinell Hardness Tester
OMEGA-HB-3000 - Digital Brinell Hardness Tester
Features
- Comprehensive Test Force Range: 62.5 to 3000 Kgf for versatile testing.
- Digital Precision: High-resolution display for accurate and easy readings.
- Durable Construction: Built to withstand rigorous testing conditions.
Technical Specifications - OMEGA-HB-3000
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 Kgf |
| Testing Range | ~8 to 650 HBW |
| Max Height of Specimen | 8.9 inches (225 mm) |
| Max Width of Specimen | 5.3 inches (135 mm) |
| Power Requirements | 110V or 220V |
| Dimensions (WxDxH) | 9.3 x 21.5 x 31.1 inches (235 x 545 x 790 mm) |
| Weight | 290 lbs (130 kg) |
| Part Number | OMEGA-HB-3000 |
OMEGA-AUTO-HB Fully Automated Brinell Hardness Tester
OMEGA-AUTO-HB - Fully Automated Brinell Hardness Tester
Features
- Automated Testing: Simplifies the testing process with fully automated load and measurement sequences.
- Wide Test Force Range: From 62.5 to 3000 Kgf, suitable for a variety of materials.
- Large Sample Capacity: Accommodates specimens up to 10 inches in height and 6 inches in width.
Technical Specifications - OMEGA-AUTO-HB
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 Kgf |
| Testing Range | ~3.2 to 650 HBW |
| Max Height of Specimen | 10 inches (260 mm) |
| Max Width of Specimen | 6 inches (150 mm) |
| Power Requirements | 110V or 220V |
| Dimensions (WxDxH) | 12 x 24.5 x 39 inches (313 x 622 x 992 mm) |
| Weight | 375 lbs (170 kg) |
| Part Number | OMEGA-AUTO-HB |