MEGA-M250S Manual Abrasive Cutter
Item ID: MEGA-M250S
An economical 10-inch manual abrasive cutter built for reliable, day-to-day metallographic sectioning. Its variable-speed motor and T-slot table handle a wide range of materials with precision.
Features
- Economical manual cutting with variable speed control
- Powerful 3-phase asynchronous motor for efficient operation
- Precise wheel feed cutting for enhanced accuracy
- Stable T-slot table fixturing for secure material placement
Technical Specifications
| Parameter | Specification |
|---|---|
| Cutting Wheel Diameter | 250 mm (~10 inches) |
| Arbor Size | 32 mm |
| Cutting Capacity (H x D) | Maximum 50 x 100 mm (2 x 4 inches) |
| Max Cutting Diameter | 75 mm (3 inches) |
| Wheel Feed | Manual |
| Vertical Movement (Z-axis) | 82 mm (3.25 inches) |
| T-slotted Table Dimensions | 250 x 230 mm (9.75 x 9 inches) |
| Motor Power | 2.2 kW (3 hp) |
| Motor Speed | Variable (300-3000 rpm) |
| Electrical Specification | 220V single phase, 380V or 480V, 3φ (50/60 Hz) |
| Cutting Force (Current Settings) | 15 amps (max) |
| Cooling Unit | 53 liters (14 gallons) |
| Dimensions (WxDxH) - Hood Closed | 750 x 685 x 720 mm (29.5 x 27 x 28 inches) |
| Dimensions (WxDxH) - Hood Open | 750 x 685 x 990 mm (29.5 x 27 x 39 inches) |
| Weight | 110 kg (240 lbs) |
| Cutter Support Bench (Optional) | MEGA-T2-BENCH |
| Catalog Number | MEGA-M250S |