TP-7500S Hydraulic Compression Mounting Press
The TP-7500S Hydraulic Compression Mounting Press ensures precise, consistent sample preparation with hydraulic pressure. It supports 1 to 2-inch mounts and features a 1600-watt heater for heating up to 392°F (200°C). Its water-cooling system with manual or automated controls makes it ideal for labs needing reliable, repeatable results.
Features
- Powerful Force Application: Uses hydraulic pressure for consistent and reliable mounting.
- Versatile Mount Sizes: Supports 1 to 2-inch (25-50 mm) molds with fixed and interchangeable cylinders.
- Robust Heating System: Features a 1600-watt heater with 110V or 220V options.
- Precise Thermal Control: Offers temperature management up to 392°F (200°C) with water-cooling options.
- Heavy-Duty Design: Handles incoming pressures up to 6460 psi for demanding applications.
Technical Specifications - TP-7500S
| Parameter | Specification |
|---|---|
| Control | Touch screen |
| Mount Sizes | 1, 1.25, 1.5, and 2-inch (25, 30, 40 mm) |
| Mold Cylinders | Single |
| Force | Hydraulic |
| Maximum Force | 32 MPa (4500 psi) |
| Heater Specification | 1000 Watts (110V 15 amp), 2000 Watts (220V 10 amp) |
| Maximum Temperature | 392°F (200°C) |
| Cooling System | Water with manual, temperature, or time control |
| Dimensions (WxDxH) | 21 x 19 x 19 inches (530 x 480 x 480 mm) |
| Weight | 108 lbs (50 kg) |
| Optional Accessory | TP-TANK Recirculating/Cooling Tank (14 gallon) with pump |
| Catalog Number | TP-7500S-110V & TP-7500S-220V |