Key Features
Wide Test Force Range
Support for test forces from 1kgf to 3000kgf, accommodating diverse material types and testing requirements across Brinell and MacroVickers methods.
Precision Optics
High-quality optical systems with multiple magnification options enable accurate indent measurement and detailed sample observation.
Automation Options
Range from manual operation to fully automated systems, providing flexibility for different testing workflows and throughput needs.
OMEGA-5000-VZ - Semi-Automated MacroVickers Hardness Tester
OMEGA-5000-VZ Semi-Automated MacroVickers Hardness Tester
Item ID: OMEGA-5000-VZ
The OMEGA-5000-VZ Semi-Automated MacroVickers Hardness Tester provides versatile testing with a test force range from 1kgf to 50kgf. With precision optics and automated shifting between objective and indenter, it streamlines testing workflows while ensuring accurate and consistent results.
Features
- Test Force Range: 1kgf to 50kgf for versatile testing needs
- Precision Optics: Includes 10X and 20X objectives for clear and detailed observations
- Automated Shifting: Automatically shifts between objective and indenter for efficient testing
Technical Specifications - OMEGA-5000-VZ
| Parameter | Specification |
|---|---|
| Test Force Range | 1kgf, 2kgf, 2.5kgf, 3kgf, 5kgf, 10kgf, 20kgf, 30kgf, 50kgf |
| Optical Magnification | 100X, 200X (10X and 20X objectives) |
| Loading Method | Automatic (Loading/Dwell/Unloading) |
| Dwell Time | Adjustable 5-60 seconds |
| Resolution | 0.25µm, 0.125µm |
| Construction | Aluminum and stainless steel |
| Maximum Sample Height | 6.7 inches (170 mm) |
| Dimensions (WxDxH) | 11 x 21 x 25 inches (280 x 530 x 630 mm) |
| Weight | 77 lbs (35 kg) |
| Part Number | OMEGA-5000-VZ |
OMEGA-HB - Manual Brinell Hardness Tester
OMEGA-HB Manual Brinell Hardness Tester
Item ID: OMEGA-HB
The OMEGA-HB Manual Brinell Hardness Tester provides robust testing capabilities with a wide test force range from 62.5 to 3000 Kgf. Equipped with a 20X optical scope and sturdy construction, it delivers reliable hardness measurements for various materials in demanding environments.
Features
- Wide Test Force Range: 62.5 to 3000 Kgf for robust testing across various materials
- Optical Measuring Device: Equipped with a 20X optical scope for accurate measurement
- Sturdy Construction: Designed for long-term durability in demanding environments
Technical Specifications - OMEGA-HB
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 Kgf |
| Optical Measuring Device | 20X Optical scope |
| Max Height of Specimen | 8.1 inches (205 mm) |
| Throat Height | 5.3 inches (135 mm) |
| Power Requirements | 110V/60 Hz; 220V/50 Hz |
| Dimensions (WxDxH) | 9.3 x 21.5 x 29.7 inches (235 x 545 x 755 mm) |
| Weight | 290 lbs (130 kg) |
| Part Number | OMEGA-HB |
OMEGA-HB-3000 - Digital Brinell Hardness Tester
OMEGA-HB-3000 Digital Brinell Hardness Tester
Item ID: OMEGA-HB-3000
The OMEGA-HB-3000 Digital Brinell Hardness Tester offers comprehensive testing capabilities with a test force range from 62.5 to 3000 Kgf. With a high-resolution digital display and durable construction, it provides accurate and easy-to-read hardness measurements for various materials.
Features
- Comprehensive Test Force Range: 62.5 to 3000 Kgf for versatile testing
- Digital Precision: High-resolution display for accurate and easy readings
- Durable Construction: Built to withstand rigorous testing conditions
Technical Specifications - OMEGA-HB-3000
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 Kgf |
| Testing Range | ~3.2 to 650 HBW |
| Max Height of Specimen | 8.8 inches (225 mm) |
| Max Width of Specimen | 5.3 inches (135 mm) |
| Power Requirements | 110V or 220V |
| Dimensions (WxDxH) | 9.3 x 21.5 x 31.1 inches (235 x 545 x 790 mm) |
| Weight | 290 lbs (130 kg) |
| Part Number | OMEGA-HB-3000 |
OMEGA-AUTO-HB - Fully Automated Brinell Hardness Tester
OMEGA-AUTO-HB Fully Automated Brinell Hardness Tester
Item ID: OMEGA-AUTO-HB
The OMEGA-AUTO-HB Fully Automated Brinell Hardness Tester simplifies the testing process with fully automated load and measurement sequences. With a test force range from 62.5 to 3000 Kgf and large sample capacity, it provides efficient, high-throughput testing for various materials.
Features
- Automated Testing: Simplifies the testing process with fully automated load and measurement sequences
- Wide Test Force Range: From 62.5 to 3000 Kgf, suitable for a variety of materials
- Large Sample Capacity: Accommodates specimens up to 10 inches in height and 6 inches in width
Technical Specifications - OMEGA-AUTO-HB
| Parameter | Specification |
|---|---|
| Test Force Range | 62.5, 100, 125, 187.5, 250, 500, 750, 1000, 1500, 3000 Kgf |
| Testing Range | ~3.2 to 650 HBW |
| Max Height of Specimen | 10 inches (260 mm) |
| Max Width of Specimen | 6 inches (150 mm) |
| Power Requirements | 110V or 220V |
| Dimensions (WxDxH) | 12 x 24.5 x 39 inches (313 x 622 x 992 mm) |
| Weight | 375 lbs (170 kg) |
| Part Number | OMEGA-AUTO-HB |