Key Features
Multiple Rockwell Scales
Support for standard Rockwell scales (HRA, HRB, HRC) and superficial scales for comprehensive hardness testing across diverse materials.
Versatile Test Forces
Configurable test forces from 15 Kgf to 150 Kgf, accommodating various material types and testing requirements.
Automation Options
Range from manual operation to fully automated systems, providing flexibility for different testing workflows and throughput needs.
OMEGA-RT - Manual Rockwell Hardness Tester
OMEGA-RT Manual Rockwell Hardness Tester
Item ID: OMEGA-RT
The OMEGA-RT Manual Rockwell Hardness Tester provides reliable hardness measurement with manual loading control. Supporting HRA, HRB, and HRC scales with test forces of 60, 100, and 150 Kgf, it offers operator-controlled precision for consistent testing results.
Features
- Rockwell Scales: HRA, HRB, HRC
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Manual Loading Control: Provides operator control for precise testing
Technical Specifications - OMEGA-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 7.2 x 21.5 x 29.7 inches (182 x 546 x 755 mm) |
| Weight | 200 lbs (90 kg) |
| Part Number | OMEGA-RT |
OMEGA-RT2 - Manual Rockwell Hardness Tester
OMEGA-RT2 Manual Rockwell Hardness Tester
Item ID: OMEGA-RT2
The OMEGA-RT2 Manual Rockwell Hardness Tester offers reliable hardness measurement with manual loading control. Supporting HRA, HRB, and HRC scales with test forces of 60, 100, and 150 Kgf, it provides operator-controlled precision for consistent testing results.
Features
- Rockwell Scales: HRA, HRB, HRC
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Manual Loading Control: Provides operator control for precise testing
Technical Specifications - OMEGA-RT2
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 9.6 x 20.5 x 27.6-inch (245 x 520 x 700mm) |
| Weight | 172 lbs (78 kg) |
| Part Number | OMEGA-RT2 |
OMEGA-DIGI-RT - Digital Rockwell Hardness Tester
OMEGA-DIGI-RT Digital Rockwell Hardness Tester
Item ID: OMEGA-DIGI-RT
The OMEGA-DIGI-RT Digital Rockwell Hardness Tester features a digital interface with automatic hardness conversion. Supporting 15 Rockwell scales (HRA through HRV) with test forces of 60, 100, and 150 Kgf, it provides easy operation and precise control for comprehensive hardness testing.
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Digital Interface: Provides easy operation and precise control with auto hardness conversion
Technical Specifications - OMEGA-DIGI-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 1-60 seconds |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 7 x 21.5 x 30 inches (182 x 546 x 755 mm) |
| Weight | 198 lbs (90 kg) |
| Part Number | OMEGA-DIGI-RT |
OMEGA-RT-60/150 - Digital Rockwell Hardness Tester
OMEGA-RT-60/150 Digital Rockwell Hardness Tester
Item ID: OMEGA-RT-60/150
The OMEGA-RT-60/150 Digital Rockwell Hardness Tester provides digital operation with support for 60 and 150 Kgf test forces. This versatile tester offers precise hardness measurements with an intuitive digital interface for efficient testing workflows.
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Digital Interface: Provides easy operation and precise control with auto hardness conversion
Technical Specifications - OMEGA-RT-60/150
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 0-60 seconds |
| Instrument Throat Height | 6.5 inches (165 mm) |
| Dimensions (WxDxH) | 8.5 x 20 x 28 inches (215 x 520 x 700 mm) |
| Weight | 172 lbs (78 kg) |
| Part Number | OMEGA-RT-60/150 |
OMEGA-AUTO-RT - Automated Rockwell Hardness Tester
OMEGA-AUTO-RT Automated Rockwell Hardness Tester
Item ID: OMEGA-AUTO-RT
The OMEGA-AUTO-RT Automated Rockwell Hardness Tester provides fully automated operation for consistent and repeatable results. Supporting 15 Rockwell scales with test forces of 60, 100, and 150 Kgf, it minimizes operator intervention while ensuring precise hardness measurements.
Features
- Rockwell Scales: HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV
- Preliminary Test Force: 10 Kgf (98.07N)
- Full Test Force: 60 Kgf, 100 Kgf, 150 Kgf
- Fully Automated Operation: Ensures consistent and repeatable results with minimal operator intervention
Technical Specifications - OMEGA-AUTO-RT
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Preliminary Test Force | 10 Kgf (98.07N) |
| Full Test Force | 60 Kgf, 100 Kgf, 150 Kgf |
| Hardness Resolution | 0.1 HR |
| Dwell Time | Adjustable 1-60 seconds |
| Instrument Throat Height | 11 inches (280 mm) |
| Dimensions (WxDxH) | 9 x 24 x 34.8 inches (225 x 615 x 885 mm) |
| Weight | 275 lbs (125 kg) |
| Part Number | OMEGA-AUTO-RT |
OMEGA-RST-15/150 - Digital Dual Rockwell / Superficial Hardness Tester
OMEGA-RST-15/150 Digital Dual Rockwell / Superficial Hardness Tester
Item ID: OMEGA-RST-15/150
The OMEGA-RST-15/150 Digital Dual Rockwell / Superficial Hardness Tester provides versatile testing capabilities for both Rockwell and Superficial Rockwell scales. With digital controls and a wide range of test forces, it offers precise and repeatable results for diverse materials and applications.
Features
- Versatile Testing: Capable of both Rockwell and Superficial Rockwell hardness testing
- Adjustable Test Forces: Offers a wide range of test forces for different materials and applications
- Digital Precision: Includes digital controls for accurate and repeatable testing results
Technical Specifications - OMEGA-RST-15/150
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV, HR15N, HR30N, HR45N, HR15T, HR30T, HR45T |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.3 inches (165 mm) |
| Dimensions (WxDxH) | 8.5 x 20 x 28 inches (215 x 520 x 700 mm) |
| Weight | 175 lbs (80 kg) |
| Part Number | OMEGA-RST-15/150 |
OMEGA-DIGI-RST - Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester
OMEGA-DIGI-RST Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester
Item ID: OMEGA-DIGI-RST
The OMEGA-DIGI-RST Digital Semi-Automated Dual Rockwell / Superficial Hardness Tester combines manual and automated features for efficient testing. With digital controls and support for both Rockwell and Superficial Rockwell scales, it provides accurate and repeatable results.
Features
- Semi-Automated Operation: Combines manual and automated features for efficient testing
- Digital Precision: Includes digital controls for accurate and repeatable testing results
- Versatile Testing: Capable of both Rockwell and Superficial Rockwell hardness testing
Technical Specifications - OMEGA-DIGI-RST
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 8.8 x 24 x 35 inches (225 x 615 x 885 mm) |
| Weight | 265 lbs (120 kg) |
| Part Number | OMEGA-DIGI-RST |
OMEGA-AUTO-RST - Automated Dual Rockwell / Superficial Hardness Tester
OMEGA-AUTO-RST Automated Dual Rockwell / Superficial Hardness Tester
Item ID: OMEGA-AUTO-RST
The OMEGA-AUTO-RST Automated Dual Rockwell / Superficial Hardness Tester provides fully automated operation for both Rockwell and Superficial Rockwell testing. Designed for high-volume testing environments, it delivers accurate and consistent results with minimal operator intervention.
Features
- Fully Automated Testing: Offers complete automation for Rockwell and Superficial Rockwell hardness testing
- High Throughput: Designed for efficient, high-volume testing environments
- Precision Control: Provides accurate and consistent results with minimal operator intervention
Technical Specifications - OMEGA-AUTO-RST
| Parameter | Specification |
|---|---|
| Rockwell Scales | HRA, HRB, HRC, HRD, HRE, HRF, HRG, HRH, HRK, HRL, HRM, HRR, HRP, HRS, HRV |
| Test Forces | 3 Kgr (Superficial), 10 Kgr (Rockwell) |
| Full Test Forces | 15, 30, 45 Kgf (Superficial); 60, 100, 150 Kgf (Rockwell) |
| Resolution | 0.1 HR |
| Instrument Throat Height | 6.9 inches (175 mm) |
| Dimensions (WxDxH) | 9 x 24 x 34.8 inches (225 x 615 x 885 mm) |
| Weight | 275 lbs (125 kg) |
| Part Number | OMEGA-AUTO-RST |