PACE Technologies' polycrystalline diamond polishing abrasives are designed for rapid material removal with minimal surface damage. Featuring a multi-faceted crystal structure, these abrasives enhance surface leveling and reduce sub-surface deformation, making them ideal for polishing hard and brittle materials.

Polycrystalline Diamond Polishing

Key Considerations

Select Appropriate Viscosity

Use high-viscosity suspensions for aggressive polishing, and low-viscosity for delicate or heat-sensitive materials.

Pair with Compatible Pads

Use low-nap or non-woven polishing pads to optimize abrasive contact and surface finish.

Adjust Force and Time

Polycrystalline diamond cuts faster, so reduce polishing time and pressure to prevent over-polishing or relief.

Introduction

Polycrystalline diamond polishing is a critical step in achieving uniform, high-quality surface finishes during metallographic sample preparation. With its multi-faceted crystal structure, polycrystalline diamond offers superior material removal rates and minimized subsurface damage, especially on hard and brittle materials. These abrasives are best used with low- to medium-napped polishing pads to maintain flatness and avoid issues like relief or edge rounding. Selecting the proper viscosity and suspension format, paired with the right cloth and lubrication, ensures efficient, reproducible polishing results for accurate microstructural analysis.

Diamond Abrasive Selection Guidelines

This reference outlines best-practice abrasive sizes for rough and final polishing across metals, ceramics, and composite materials. Proper abrasive selection is critical to ensure accurate microstructural representation, prevent surface damage, and optimize polishing efficiency.

Preferred Abrasive
Acceptable Alternative
Not Typically Recommended

Polishing Guide for Metals

Metal Rough Polishing (Diamond) Final Polishing (Oxide)
Abrasive Size 9 µm 6 µm 3 µm 1 µm Al2O3 SiO2
Aluminum
Copper / Brass
Stainless Steel
Soft Steel
Hard Steel
Tool Steel
Titanium Etch Polish
Zinc, Tin, Lead

Polishing Guide for Ceramics and Composites

Ceramic / Composite Coarse Grind Fine Grind Rough Polish Fine Polish
Diamond Size 30 µm 15 µm 9 µm 6 µm 3 µm 1 µm + SiO2
Alumina
Silicon Nitride
Polymer Composite
Metal Matrix Composite
Ceramic Matrix Composite
Cermet

Note: These selections reflect proven laboratory procedures balancing speed, flatness, and structure preservation. Adjust abrasive types and sequence for material-specific variables such as grain size, hardness, and thermal sensitivity.

Polymer composites: Diamond can embed in soft polymer matrices and carry through to subsequent steps. For polymer-dominated samples, SiC grinding (through P2400 or P4000) followed directly by alumina or colloidal silica is often preferred. Reserve diamond polishing for fiber- or filler-dominated composites where the matrix can tolerate it.

Polishing Pad Selection Guideline

Pad Image & Link Use Case Pad Icon Polishing Stage
CERMESH CERMESH metal mesh pad used for semi-fixed abrasive coarse to intermediate lapping. Excellent for initial removal of damage from sectioning and hard materials. CERMESH icon Coarse / Intermediate
POLYPAD POLYPAD is a durable synthetic polyester pad ideal for intermediate polishing, especially with 6-15 µm diamond abrasives. Designed as a long-life nylon alternative. POLYPAD icon Intermediate
TEXPAN TEXPAN is a widely used non-woven intermediate polishing pad, compatible with most diamond suspensions. Effective across a broad range of materials. TEXPAN icon Intermediate
Black CHEM 2 Black CHEM 2 is a porometric polymer pad with rubber-like consistency, offering balanced action between low and high nap pads. Ideal for moderate nap intermediate polishing. Black CHEM 2 icon Intermediate
DACRON II DACRON II is a non-napped woven polishing pad widely used in Europe for intermediate steps on metals. Suitable for 1-15 µm diamond abrasives. DACRON icon Intermediate
NYPAD NYPAD is a low-napped nylon pad tailored for intermediate polishing of harder metals and alloys. Performs well with mid-size diamond abrasives. NYPAD icon Intermediate
GOLD PAD GOLD PAD is a low-napped pad ideal for 1-9 µm polishing. Designed for consistent material removal and flatness control during final pre-polishing. GOLD PAD icon Intermediate
ATLANTIS ATLANTIS is a woven low-nap final polishing pad with foam backing for enhanced compliance. Ideal for 1-6 µm diamond. Great for critical surface flatness needs. ATLANTIS icon Final
MICROPAD MICROPAD is a high-napped final polishing pad ideal for producing a mirror finish on metals and polymers. Recommended for <1 µm diamond or colloidal silica. MICROPAD icon Final
TRICOTE TRICOTE is a tight high-napped final polishing pad for metals. Offers better control of surface texture and minimal abrasive drag. TRICOTE icon Final
NAPPAD NAPPAD is a very high-napped final polishing pad tailored for soft metals and polymers. Provides gentle polishing action to minimize pull-out and relief. NAPPAD icon Final
MOLTEC 2 MOLTEC 2 is a wool-based final polishing cloth used when edge retention is not critical. Works well with alumina and colloidal silica on metals. MOLTEC icon Final
FELT PAD FELT PAD is a thick final polishing pad made for large samples or glass. Ideal for use with colloidal silica or alumina slurries where surface uniformity is key. FELT PAD icon Final
View collection →

Process Description

Polycrystalline diamond polishing is typically performed in one or two stages depending on material hardness and surface condition. For rough polishing, low- to medium-napped pads are used with coarse polycrystalline diamond suspensions or pastes to efficiently remove grinding damage. In many cases, this may be followed by a finer grade of polycrystalline diamond for surface refinement. Due to the abrasive’s multi-crystalline nature, material removal is rapid yet controlled, minimizing heat and deformation. Excessive polishing should be avoided to prevent artifacts such as relief, smear, or rounding.

Minimizing Polishing Artifacts

To prevent common polishing issues such as edge rounding, relief, or abrasive embedding:

  • Use polycrystalline diamond suspensions with the correct viscosity for your application
  • Select low-napped pads to maintain surface flatness during rough polishing
  • Ensure polishing plates have minimal runout (≤0.0001" / 2.5 µm for 8" platens)
  • Use moderate force and avoid prolonged polishing times
Maintaining a flat and stable polishing surface is crucial for consistency and minimizing microstructural distortion.

Recommended Procedures

  • Secure the polishing pad firmly to a flat platen (adhesive or magnetic backing as appropriate)
  • Pre-wet and pre-charge the pad with polycrystalline diamond suspension or paste
  • Apply the recommended lubricant to optimize cutting and prevent pad clogging
  • Start polishing with reduced downforce to avoid premature pad wear or sample relief
  • At the end of the step, rinse the specimen thoroughly with water followed by ethanol before drying
  • Clean and dry specimens thoroughly to remove all residues before inspection

Polycrystalline Diamond Suspensions (water-based)

Description Quantity Low Viscosity High Viscosity Product Image
0.05 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-0105-250
GPC-0105-500
GPC-0105-1GL
PC-0105-250
PC-0105-500
PC-0105-1GH
PACE Technologies 0.05 micron polycrystalline diamond suspension
0.1 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-0110-250
GPC-0110-500
GPC-0110-1GL
PC-0110-250
PC-0110-500
PC-0110-1GH
PACE Technologies 0.1 micron polycrystalline diamond suspension
0.25 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-0125-250
GPC-0125-500
GPC-0125-1GL
PC-0125-250
PC-0125-500
PC-0125-1GH
PACE Technologies 0.25 micron polycrystalline diamond suspension
0.5 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-0150-250
GPC-0150-500
GPC-0150-1GL
PC-0150-250
PC-0150-500
PC-0150-1GH
PACE Technologies 0.50 micron polycrystalline diamond suspension
1 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1001-250
GPC-1001-500
GPC-1001-1GL
PC-1001-250
PC-1001-500
PC-1001-1GH
PACE Technologies 1 micron polycrystalline diamond suspension
3 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1003-250
GPC-1003-500
GPC-1003-1GL
PC-1003-250
PC-1003-500
PC-1003-1GH
PACE Technologies 3 micron polycrystalline diamond suspension
6 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1006-250
GPC-1006-500
GPC-1006-1GL
PC-1006-250
PC-1006-500
PC-1006-1GH
PACE Technologies 6 micron polycrystalline diamond suspension
9 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1009-250
GPC-1009-500
GPC-1009-1GL
PC-1009-250
PC-1009-500
PC-1009-1GH
PACE Technologies 9 micron polycrystalline diamond suspension
15 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1015-250
GPC-1015-500
GPC-1015-1GL
PC-1015-250
PC-1015-500
PC-1015-1GH
PACE Technologies 15 micron polycrystalline diamond suspension
30 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1030-250
GPC-1030-500
GPC-1030-1GL
PC-1030-250
PC-1030-500
PC-1030-1GH
PACE Technologies 30 micron polycrystalline diamond suspension
45 micron DIAMAT Polycrystalline diamond 250 ml
500 ml
1 gallon
GPC-1045-250
GPC-1045-500
GPC-1045-1GL
PC-1045-250
PC-1045-500
PC-1045-1GH
PACE Technologies 45 micron polycrystalline diamond suspension

Polycrystalline Diamond Suspension - Dyed

Description Quantity Catalog Number Product Image
1 micron (blue) DIAMAT PC Suspension 1 liter PC-1001-1L 1 micron dyed PC diamond suspension
1 micron (blue) DIAMAT PC Suspension 1 gallon PC-1001-1GLB
3 micron (green) DIAMAT PC Suspension 1 liter PC-1003-1L 3 micron dyed PC diamond suspension
3 micron (green) DIAMAT PC Suspension 1 gallon PC-1003-1GLG
6 micron (yellow) DIAMAT PC Suspension 1 liter PC-1006-1L 6 micron dyed PC diamond suspension
6 micron (yellow) DIAMAT PC Suspension 1 gallon PC-1006-1GLY
9 micron (red) DIAMAT PC Suspension 1 liter PC-1009-1L 9 micron dyed PC diamond suspension
9 micron (red) DIAMAT PC Suspension 1 gallon PC-1009-1GLR
15 micron (brown) DIAMAT PC Suspension 1 liter PC-1015-1L 15 micron dyed PC diamond suspension
15 micron (brown) DIAMAT PC Suspension 1 gallon PC-1015-1GLBR
30 micron (orange) DIAMAT PC Suspension 1 liter PC-1030-1L 30 micron dyed PC diamond suspension
30 micron (orange) DIAMAT PC Suspension 1 gallon PC-1030-1GLO
45 micron (purple) DIAMAT PC Suspension 1 liter PC-1045-1L 45 micron dyed PC diamond suspension
45 micron (purple) DIAMAT PC Suspension 1 gallon PC-1045-1GLP

Polycrystalline Diamond Paste

Description Quantity Catalog Number Product Image
DIAMAT Polycrystalline Diamond Paste (0.1 µm) 5 gm
20 gm
PC-0210-05
PC-0210-20
0.1 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (0.25 µm) 5 gm
20 gm
PC-0225-05
PC-0225-20
0.25 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (0.5 µm) 5 gm
20 gm
PC-0250-05
PC-0250-20
0.5 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (1 µm) 5 gm
20 gm
PC-2001-05
PC-2001-20
1 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (3 µm) 5 gm
20 gm
PC-2003-05
PC-2003-20
3 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (6 µm) 5 gm
20 gm
PC-2006-05
PC-2006-20
6 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (9 µm) 5 gm
20 gm
PC-2009-05
PC-2009-20
9 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (15 µm) 5 gm
20 gm
PC-2015-05
PC-2015-20
15 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (30 µm) 5 gm
20 gm
PC-2030-05
PC-2030-20
30 micron polycrystalline diamond paste
DIAMAT Polycrystalline Diamond Paste (45 µm) 5 gm
20 gm
PC-2045-05
PC-2045-20
45 micron polycrystalline diamond paste

Diamond Extenders (Lubricants)

Description Quantity Catalog Number Product Image
DIALUBE Diamond Extender 16 oz (0.125L)
32 oz (0.24L)
1 gallon (3.8L)
DL-3000-16
DL-3000-32
DL-3000-128
Metallographic diamond polishing lubricants
DIALUBE Blue Alcohol Lubricant 16 oz (0.125L)
32 oz (0.24L)
1 gallon (3.8L)
AOD-3000-16
AOD-3000-32
AOD-3000-128
DIALUBE Purple Alcohol Lubricant 16 oz (0.125L)
32 oz (0.24L)
1 gallon (3.8L)
ADL-3000-16
ADL-3000-32
ADL-3000-128
POLYLUBE Non-Aqueous Diamond Extender 16 oz (0.125L)
32 oz (0.24L)
1 gallon (3.8L)
PDL-3000-16
PDL-3000-32
PDL-3000-128
POLYLUBE Red (Anti-Corrosion) Lube 16 oz (0.125L)
32 oz (0.24L)
1 gallon (3.8L)
PDL-3000R-16
PDL-3000R-32
PDL-3000R-128

Troubleshooting

Symptom Cause Solution
Coarse Scratching Contaminated polishing pad or incorrect pad pairing Replace pad; use correct pad type for polycrystalline diamond
Agglomerated Diamond Pre-mixing with colloidal silica; bacterial growth in suspension Dispense abrasives separately; replace suspension if contaminated
Uneven Polishing Worn pad or uneven platen surface Replace pad; check and resurface platen if needed
Edge Rounding / Excessive Relief Too much downforce or extended polishing duration Reduce force; shorten polishing time; verify prior steps were sufficient
Low Polishing Rate Insufficient abrasive concentration or poor pad saturation Increase suspension application rate; recharge pad with diamond
Tearing of Pad High pressure or inadequate lubrication Lower pressure; apply lubricant more frequently
Specimen Smear or Pull-Out Inappropriate pad or overly aggressive abrasive size Use lower nap pad and finer diamond grit; evaluate pad compatibility

Related Equipment

Frequently Asked Questions

Common questions about polycrystalline diamond polishing

What is the difference between polycrystalline and monocrystalline diamond?

Polycrystalline diamond consists of many small diamond crystals, providing multiple cutting edges for faster material removal. Monocrystalline diamond has single crystal structure with consistent geometry, offering more controlled and finer polishing. Polycrystalline is preferred for rough polishing and hard materials, while monocrystalline excels at final polishing for superior surface finish.

Which materials benefit most from polycrystalline diamond polishing?

Polycrystalline diamond is ideal for hard and tough materials including tool steels, carbides, ceramics, cermets, and composite materials. It removes grinding damage quickly on materials that would take excessive time with conventional abrasives. For softer metals like aluminum or copper, consider finer polycrystalline grades or switch to monocrystalline diamond to avoid excessive material removal.

What viscosity should I use - suspension, paste, or spray?

Suspensions (low viscosity) provide excellent lubrication and heat dissipation, ideal for automated systems and extended polishing. Pastes (high viscosity) offer concentrated abrasive delivery and longer pad life, preferred for manual polishing or when frequent recharging is impractical. Sprays provide light, controlled application for final polishing steps. Choose based on equipment type, material, and desired convenience.

How do I prevent over-polishing with polycrystalline diamond?

Polycrystalline diamond cuts aggressively, so reduce polishing time and pressure compared to conventional abrasives. Start with shorter polishing intervals (1-2 minutes) and inspect frequently. Use low-nap or non-woven pads to minimize embedment. Monitor for signs of relief, rounding, or smearing. Once grinding damage is removed, transition to finer grades or monocrystalline diamond rather than continuing with the same abrasive.

What polishing pad should I use with polycrystalline diamond?

For rough polishing with coarse polycrystalline diamond (15-9 µm), use low-nap pads like POLYPAD or GOLDPAD, or a CERMESH metal mesh for fixed-abrasive lapping on hard materials. For intermediate polishing (6-3 µm), use non-woven or low-nap pads like TEXPAN, DACRON II, or Black CHEM 2. Reserve high-nap cloths like MICROPAD and NAPPAD for final polishing with sub-micron diamond or colloidal silica; using them with coarser diamond causes excessive embedment and edge rounding.

Can I use polycrystalline diamond for final polishing?

Polycrystalline diamond can be used for final polishing with 1-3 µm grades on very hard materials where conventional alumina polishing is ineffective. However, for most materials, monocrystalline diamond (1 µm or 0.25 µm) or colloidal silica provides superior final surface finish with less risk of artifacts. Reserve polycrystalline for rough and intermediate stages, then transition to finer abrasives for the final step.