Technical Specifications
| Parameter | Specification |
|---|---|
| Cutting Wheel Diameter | 250 mm (~10 inches) |
| Arbor Size | 32 mm |
| Cutting Capacity (H x D) | Maximum 50 x 200 mm (2 x 8 inches) |
| Max Cutting Diameter | 75 mm (3 inches) |
| Wheel Feed | Manual |
| Table Feed | Manual |
| Y Pulse Feed | Manual |
| Y Constant Feed | Manual |
| Vertical Movement (Z-axis) | 100 mm (3.9 inches) |
| Table Feed Movement (Y-axis) | 100 mm (4 inches) |
| T-slotted Table Dimensions | 280 x 470 mm (11 x 18.25 inches) |
| Motor Power | 4.5 kW (6 hp) |
| Motor Speed | Variable (1500-3500 rpm) |
| Electrical Specification | 208Y / 380V or 480V, 3φ (50/60 Hz) |
| Cutting Force (Current Settings) | 3-15 amps (Adjustable) |
| Cooling Unit | 53 liters (14 gallons) |
| Dimensions (WxDxH) - Hood Closed | 900 x 815 x 710 mm (35.5 x 32 x 28 inches) |
| Dimensions (WxDxH) - Hood Open | 900 x 815 x 990 mm (35.5 x 32 x 39 inches) |
| Weight | 171 kg (377 lbs) |
| Cutter Support Bench (Optional) | MEGA-T2-BENCH |
| Catalog Number | MEGA-T250S |