TP-7100S Pneumatic Compression Mounting Press
Item ID: TP-7100S
A pneumatic compression mounting press with touchscreen control, 1600-watt heater, and interchangeable mold cylinders from 1 to 2 inches. Delivers consistent force and precise temperature control up to 392°F (200°C) for uniform metallographic mounts.
Features
- Pneumatic force for consistent, uniform mounting results
- Interchangeable 1 to 2-inch (25-50 mm) mold cylinders
- 1600-watt heater with thermostat up to 392°F (200°C)
- Touchscreen interface with programmable cycles
Technical Specifications
| Parameter | Specification |
|---|---|
| Control | Touch screen |
| Mount Sizes | 1, 1.25, 1.5, and 2-inch (25, 30, 40 mm) |
| Mold Cylinders | Single |
| Force | Pneumatic |
| Incoming Pressure | Max. 95 psi |
| Heater Specification | 1000 Watts (110V 15 amp) or 2000 Watts (110V 20 amp) |
| Maximum Temperature | 392°F (200°C) |
| Cooling System | Water with manual, temperature, or time control |
| Dimensions (WxDxH) | 21 x 19 x 19 inches (530 x 480 x 480 mm) |
| Weight | 69 lbs (32 kg) |
| Optional Accessory | TP-TANK Recirculating/Cooling Tank (14 gallon) with pump |
| Catalog Number | TP-7100S-110V & TP-7100S-220V |