Skip to main content

TP-7100S Pneumatic Compression Mounting Press

Item ID: TP-7100S

A pneumatic compression mounting press with touchscreen control, 1600-watt heater, and interchangeable mold cylinders from 1 to 2 inches. Delivers consistent force and precise temperature control up to 392°F (200°C) for uniform metallographic mounts.

Features

  • Pneumatic force for consistent, uniform mounting results
  • Interchangeable 1 to 2-inch (25-50 mm) mold cylinders
  • 1600-watt heater with thermostat up to 392°F (200°C)
  • Touchscreen interface with programmable cycles

Technical Specifications

Parameter Specification
Control Touch screen
Mount Sizes 1, 1.25, 1.5, and 2-inch (25, 30, 40 mm)
Mold Cylinders Single
Force Pneumatic
Incoming Pressure Max. 95 psi
Heater Specification 1000 Watts (110V 15 amp) or 2000 Watts (110V 20 amp)
Maximum Temperature 392°F (200°C)
Cooling System Water with manual, temperature, or time control
Dimensions (WxDxH) 21 x 19 x 19 inches (530 x 480 x 480 mm)
Weight 69 lbs (32 kg)
Optional Accessory TP-TANK Recirculating/Cooling Tank (14 gallon) with pump