A hydraulic compression mounting press with touchscreen control, 1600-watt heater, and water-cooling system for 1 to 2-inch mounts. Delivers up to 6460 psi of force with precise temperature control up to 392°F (200°C).

Features

  • Hydraulic pressure up to 6460 psi for demanding applications
  • Interchangeable 1 to 2-inch (25-50 mm) mold cylinders
  • 1600-watt heater with water-cooling system
  • Touchscreen interface with programmable cycles

Technical Specifications

Parameter Specification
Control Touch screen
Mount Sizes 1, 1.25, 1.5, and 2-inch (25, 30, 40, 50 mm)
Mold Cylinders Single
Force Hydraulic
Maximum Force 44.5 MPa (6460 psi)
Heater Specification 1600 Watts
Maximum Temperature 392°F (200°C)
Cooling System Water with manual, temperature, or time control
Dimensions (WxDxH) 21 x 19 x 19 inches (530 x 480 x 480 mm)
Weight 108 lbs (50 kg)
Optional Accessory TP-TANK Recirculating/Cooling Tank (14 gallon) with pump