FEMTO Series Autopolisher Heads
Precise and consistent polishing for metallographic sample preparation. Available in individual force and central/individual force configurations.
FEMTO-1100S - Individual Force Autopolishing Head
FEMTO-1100S Individual Force Autopolishing Head
Item ID: FEMTO-1100S
An individual force autopolishing head with 0.54 hp servo motor and variable speed up to 300 rpm. Handles 1-6 samples with individual piston force on NANO-1000S/2000S polishers.
Features
- Individual piston force for 1-6 samples
- 0.54 hp dynamic torque servo motor (0-300 rpm)
- Compatible with NANO-1000S / NANO-2000S polishers
- 110V or 220V, 50/60 Hz
Technical Specifications - FEMTO-1100S
| Parameter | Specification |
|---|---|
| Application of Force | Individual pistons (1-6 samples) |
| Head Speed | 0-300 rpm (variable) |
| Motor | 0.54 hp (400 W) dynamic torque servo motor |
| Compatibility | NANO-1000S / NANO-2000S polishers |
| Electrical Specifications | 110V or 220V 50/60 Hz |
| Part Number | FEMTO-1100S |
FEMTO-1500S - Individual / Central Force Autopolishing Head
FEMTO-1500S Individual / Central Force Autopolishing Head
Item ID: FEMTO-1500S
A dual-mode autopolishing head with both individual (1-6 samples) and central force (3-6 samples) options. Pairs with NANO-1000S/2000S polishers at up to 300 rpm.
Features
- Individual (1-6 samples) and central force (3-6 samples) modes
- 0.54 hp dynamic torque servo motor (0-300 rpm)
- Compatible with NANO-1000S / NANO-2000S polishers
- 110V or 220V, 50/60 Hz
Technical Specifications - FEMTO-1500S
| Parameter | Specification |
|---|---|
| Application of Force | Individual pistons (1-6 samples), Central force (3-6 samples) |
| Head Speed | 0-300 rpm (variable) |
| Motor | 0.54 hp (400 W) dynamic torque servo motor |
| Compatibility | NANO-1000S / NANO-2000S polishers |
| Electrical Specifications | 110V or 220V 50/60 Hz |
| Part Number | FEMTO-1500S |
FEMTO-2200S - Individual Force Autopolishing Head
FEMTO-2200S Individual Force Autopolishing Head
Item ID: FEMTO-2200S
An individual force autopolishing head designed for the NANO-1200S polisher. Provides precise piston-based force control for up to 6 samples at variable speeds up to 300 rpm.
Features
- Individual piston force for 1-6 samples
- 0.54 hp dynamic torque servo motor (0-300 rpm)
- Designed for NANO-1200S polisher
- 110V or 220V, 50/60 Hz
Technical Specifications - FEMTO-2200S
| Parameter | Specification |
|---|---|
| Application of Force | Individual pistons (1-6 samples) |
| Head Speed | 0-300 rpm (variable) |
| Motor | 0.54 hp (400 W) dynamic torque servo motor |
| Compatibility | NANO-1200S polisher |
| Electrical Specifications | 110V or 220V 50/60 Hz |
| Part Number | FEMTO-2200S |
FEMTO-2500S - Individual / Central Force Autopolishing Head
FEMTO-2500S Individual / Central Force Autopolishing Head
Item ID: FEMTO-2500S
A dual-mode autopolishing head for the NANO-1200S with individual (1-6 samples) and central force (3-12 samples) options. Variable speed up to 300 rpm with 0.54 hp servo motor.
Features
- Individual (1-6 samples) and central force (3-12 samples) modes
- 0.54 hp dynamic torque servo motor (0-300 rpm)
- Designed for NANO-1200S polisher
- 110V or 220V, 50/60 Hz
Technical Specifications - FEMTO-2500S
| Parameter | Specification |
|---|---|
| Application of Force | Individual pistons (1-6), Central force (3-12 samples) |
| Head Speed | 0-300 rpm (variable) |
| Motor | 0.54 hp (400 W) dynamic torque servo motor |
| Compatibility | NANO-1200S polisher |
| Electrical Specifications | 110V or 220V 50/60 Hz |
| Part Number | FEMTO-2500S |