PICO-200S Manual Table Feed Precision Wafering Saw
Item ID: PICO-200S
A compact manual table-feed saw for precision sectioning of small samples. Supports 6-8" blades at 500-3000 rpm with immersion cooling and dual vises.
Features
- Compact design ideal for laboratory use
- Up to 1-inch (30 mm) cutting capacity with table feed
- Continuously adjustable speed (500-3000 rpm) with electronic display
- Integrated 2.5-liter coolant tank for effective heat management
Technical Specifications
| Parameter | Specification |
|---|---|
| Cut-off Blade Size | Max. diameter 200 mm (8 inches) |
| Cutting Capacity | 30 mm (1-inch) |
| Specimen Feed | Table feed |
| Coolant Tank | 2.5 Liters |
| Arbor Size | 12.7 mm (0.5 inches) |
| Variable Speed (RPM) | 500-3000 rpm continuously adjustable with electronic speed display |
| Motor Power | 400 W |
| Electrical Specification | 110V/220V (50/60 Hz) |
| Dimensions (WxDxH) | Hood closed: 18.5 x 20 x 14-inch (47 x 50.5 x 36 cm) / Hood open: 18.5 x 22 x 25-inch (47 x 56 x 63 cm) |
| Weight | 45 kg (100 lbs) |
| Catalog Number | PICO-200S |