ASTM E10

Standard Test Method for Brinell Hardness of Metallic Materials

ASTM
Testing hardness brinell testing

Description

Test method for Brinell hardness testing. Includes procedures, indenter specifications, test forces, and measurement requirements.

Standard Information

Standard:ASTM E10
Organization:ASTM
Category:Testing