Standard Test Methods for Determining Average Grain Size

ASTM
Analysis grain-size analysis measurement planimetric intercept

Description

Methods for determining average grain size using comparison charts, planimetric (Jeffries) method, and intercept method. Includes procedures for different grain structures.

Standard Information

Standard:ASTM E112
Organization:ASTM
Category:Analysis