Practice for preparing sulfur prints for macrostructural examination. Procedures for revealing sulfur distribution in steel and other materials.
ASTM E1180
Standard Practice for Preparing Sulfur Prints for Macrostructural Examination
ASTM
Etching
sulfur-prints
macrostructural
etching
steel
Description
Standard Information
Standard:ASTM E1180
Organization:ASTM
Category:Etching