ASTM E2014

Standard Guide for Preparation of Plastics and Polymeric Specimens for Microstructural Examination

ASTM
Preparation preparation plastics polymers specimen

Description

Guide for preparing plastics and polymeric materials for microstructural examination. Covers sectioning, mounting, polishing, and etching techniques.

Standard Information

Standard:ASTM E2014
Organization:ASTM
Category:Preparation