Guide for preparing plastics and polymeric materials for microstructural examination. Covers sectioning, mounting, polishing, and etching techniques.
ASTM E2014
Standard Guide for Preparation of Plastics and Polymeric Specimens for Microstructural Examination
ASTM
Preparation
preparation
plastics
polymers
specimen
Description
Standard Information
Standard:ASTM E2014
Organization:ASTM
Category:Preparation