PACE Technologies logo PACE Technologies web collage PACE Technologies best price guarantee logo



Click here to get a quote

Metallographic Rockwell Hardness Testers

Hardness Tester Rockwell Superficial
Rockwell
Dual Superficial
Rockwell
Manual OMEGA-RT OMEGA-ST  
Standard OMEGA
RT-60/150
  OMEGA
SRT-15/150
Semi-automated OMEGA
DIGI-RT
  OMEGA
DIGI-RST
Automated OMEGA
AUTO-RT
OMEGA
AUTO-ST
OMEGA
AUTO-RST

Rockwell Hardness Testers

Manual Rockwell Hardness Tester (OMEGA-RT)

The OMEGA-RT is a basic low cost manual Rockwell hardness tester (Part No. OMEGA-RT) designed to evaluate metallographic specimen hardness.

Manual Rockwell hardness tester Metallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-RT
Rockwell Scales HRA, HRB,HRC
Preliminary test force 10 Kgr (98.07N)
Full test force 60 Kgf, 100 Kgr, 150 Kgf
Loading control manual
Instrument Throat Height 6.5-inch (165 mm)
Dimensions (W x D x H) 7.2 x 21.5 x 29.7 inch
(182 x 546 x 755mm)
Weight 200 lbs (90 kg)

Digital Rockwell Hardness Tester (OMEGA-RT-60/150)

The OMEGA-RT-60/150 is a semi-automated digital Rockwell hardness tester (Part No. OMEGA-RT-60/150) designed to evaluate metallographic specimen hardness.

Rockwell hardness tester Metallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-RT-60/150
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 10 Kgr (98.07N)
Full test force 60 Kgf, 100 Kgr, 150 Kgf
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRA, HRB, HRC, HRF,
HV, HK, HBW, HT15N,
HR30N, HR45N, HR15T,
HR30T, HR45T
Illumination Halogen (LED optional)
Instrument Throat Height 6.3-inch (160 mm)
Power 110 or 220V
Dimensions (W x D x H) 8.5 x 20 x 28 inch
(216 x 508 x 711mm)
Weight 200 lbs (90 kg)

Digital Semi-Automated Rockwell Hardness Tester (OMEGA-DIGI-RT)

OMEGA-DIGI-RT is a semi-automated digital Rockwell hardness tester The OMEGA-DIGI hardness testers are designed to evaluate metallographic specimen Rockwell hardness.

Rockwell hardness tester Metallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-DIGI-RT
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 10 Kgr (98.07N)
Full test force 60 Kgf, 100 Kgr, 150 Kgf
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HV, HBS, HBW, HK,
HRA, HRD, HR15N, HR30N,
HR45N, HS, HRF, HR15T,
HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 7 x 21.5 x 30 inches
(182 x 546 x 755 mm)
Weight 265 lbs (120 Kg)

Automated Rockwell Hardness Tester (OMEGA-AUTO-RT)

OMEGA-AUTO-RT is an automated digital Rockwell hardness tester The OMEGA-AUTO-RT hardness testers are designed to evaluate metallographic specimen Rockwell hardness.

Automated Rockwell hardness tester Metallographic Automated Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-AUTO-RT
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 10 Kgr (98.07N)
Full test force 60 Kgf, 100 Kgr, 150 Kgf
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HV, HBS, HBW, HK,
HRA, HRD, HR15N, HR30N,
HR45N, HS, HRF, HR15T,
HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 11 inches (280 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 275.6 lbs (125 Kg)

Superficial Rockwell Hardness Testers

Manual Superficial Rockwell Hardness Tester (OMEGA-ST)

The OMEGA-ST is a basic low cost manual Superficial Rockwell hardness tester (Part No. OMEGA-ST) designed to evaluate metallographic specimen hardness.

Manual Superficial Rockwell hardness tester Metallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-ST
Rockwell Scales HR15N, HR30N, HR45N,
HR15T, HR30T, HR45T
Preliminary test force 3 Kgf (29.4N)
Full test force 15 Kgf, 30 Kgr, 45 Kgf
Loading control manual
Instrument Throat Height 6.5-inch (165 mm)
Dimensions (W x D x H) 7.2 x 21.5 x 29.7 inch
(182 x 546 x 755mm)
Weight 200 lbs (90 kg)

Automated Superficial Rockwell Hardness Tester (OMEGA-AUTO-ST)

OMEGA-AUTO-ST is an automated digital Superficial Rockwell hardness tester The OMEGA-AUTO-ST hardness testers are designed to evaluate metallographic specimen Superficial Rockwell hardness.

Superficial Rockwell hardness testerMetallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-AUTO-ST
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 3 Kgr (29.4N)
Full test force 15 Kgf, 30 Kgr, 45 Kgf
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HV, HBS, HBW, HK,
HRA, HRD, HR15N, HR30N,
HR45N, HS, HRF, HR15T,
HR30T, HR45T, HRB
Illumination Halogen
Max Height of Specimen 11 inches (280 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 275.6 lbs (125 Kg)

Dual Rockwell / Superficial Rockwell Hardness Testers

Digital Dual Rockwell / Superficial Rockwell Hardness Tester (OMEGA-SRT-15/150)

The OMEGA-SRT-15/150 is an automated digital Rockwell / Superficial Rockwell Testing machine (Part No. OMEGA-SRT-15/150) designed for evaluating metallographic specimen hardness.

Superficial Rockwell hardness testerMetallographic Superficial Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-SRT-15/150
Rockwell Scales HRA, HRB, HRC, HRD, HRE,
HRF, HRG,HRH, HRK, HRL,
HRM, HRR, HRP, HRS, HRV,
HR15N, HR30N, HR45N,
HR15T, HR30T, HR45T
Preliminary test force 3 Kgr (Superficial)
10 Kgr (Rockwell)
Full test force 15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HRB, HRA, HV
HK, HBW
Illumination Halogen (LED optional)
Instrument Throat Height 6.3-inch (160 mm)
Power 110 or 220V
Dimensions (W x D x H) 7 x 21.5 x 30 inches
(182 x 546 x 755 mm)
Weight 200 lbs (90 kg)

Digital Semi-Automated Dual Rockwell/ Superficial Hardness Tester (OMEGA-DIGI-RST)

OMEGA-DIGI-RST is a semi-automated digital dual Rockwell/ Superficial Rockwell hardness tester. The OMEGA-DIGI semi-automated hardness testers are designed to evaluate metallographic specimen Rockwell and Superficial Rockwell hardness.

Rockwell hardness tester Metallographic dual Superficial and Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-DIGI-RST
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 3 Kgr (Superficial)
10 Kgr (Rockwell)
Full test force 15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HV, HBS, HBW, HK,
HRA, HRD, HR15N, HR30N,
HR45N, HS, HRF, HR15T,
HR30T, HR45T, HRB
Illumination Halogen (LED optional)
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 265 lbs (120 Kg)

Digital Automated Dual Rockwell/ Superficial Hardness Tester (OMEGA-AUTO-RST)

OMEGA-AUTO-RST is an automated digital dual Rockwell/ Superficial Rockwell hardness tester. The OMEGA-AUTO-RST hardness testers are designed to evaluate metallographic specimen Rockwell and Superficial Rockwell hardness.

Rockwell hardness tester Metallographic Rockwell Hardness Tester Click here to get a quote
Feature OMEGA-AUTO-RST
Rockwell Scales HRA, HRB,HRC,HRD,HRE,
HRF, HRG,HRH,HRK,HRL,
HRM, HRR, HRP, HRS,HRV
Preliminary test force 3 Kgr (Superficial)
10 Kgr (Rockwell)
Full test force 15 Kgf, 30 Kgr, 45 Kgr (Superficial)
60 Kgf, 100 Kgr, 150 Kgf (Rockwell)
Hardness resolution 0.1 HR
Dwell time Adjustable 1-60 seconds
Auto Hardness conversion HRC, HV, HBS, HBW, HK,
HRA, HRD, HR15N, HR30N,
HR45N, HS, HRF, HR15T,
HR30T, HR45T, HRB
Illumination Halogen (LED optional)
Max Height of Specimen 6.9-inch (175 mm)
Power 110 or 220V
Dimensions (W x D x H) 9 x 24 x 34.8 inches
(225 x 615 x 885 mm)
Weight 265 lbs (120 Kg)

PACE TECHNOLOGIES CONTACT


PACE Technologies
3601 E. 34th St.
Tucson, Arizona 85713
+1-520-882-6598
FAX +1-520-882-6599
email: pace@metallographic.com
www.metallographic.com


Information Requests

*Required Information

*Company:
*Name:
*E-mail:
Title:
*Address:
P.O. / Suite:
*City:
*State:
*Zip Code:
Country:
*Phone:
Fax:

Industry:

Process Type:

Send Equipment Quotes
Add my name to PACE Technologies mailing list
Send NEW 2018-2020 Product catalog
Send me my FREE MET MANUAL
Request a salesperson call

Metallographic
Consumables

Brochures:

For online
ordering
click here
Online Ordering
Abrasive Blades
Diamond Blades
Compression Mounting
Castable Mounting
Polishing Pads
Lapping Films
Diamond Disks
Composite Disks
Polycrystalline Diamond
Monocrystalline Diamond
Final Polishing Abrasives
Etchants
Consumables Catalog

Metallographic
Equipment

Brochures:

For specific
equipment quotes
click here
Quotes
Abrasive Cutters
Precision Wafering Saws
Compression Mounting Presses
Castable Vacuum Chamber
Manual Roll and Belt Grinders
Polishing Machines
Automated Polishing Heads
Vibratory Polisher

Metallographic
Analysis
Brochures:

For specific
instrument quotes
click here
Quotes
Microscopes
Microhardness Testers
Rockwell Hardness Testers
Brinell Hardness Testers
MacroVickers Hardness Tester
Image Analysis

Laboratory
Furniture
Brochures:

For specific
items quotes
click here
Quotes
Lab Benches
Microscope Benches
Fume Hood
Safety Cabinets
Specimen Storage Cabinet

Other Questions

Question To:
Enter Request Info. or Question:



Copyright 2006-2019
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies Google+ PACE Technologies Google+