Description:
Ceramics in general are relatively brittle with a wide range of thermal and hardness characteristics.

Preparation Challenge:
Proper specimen preparation requires that grinding damage be minimized as early as possible followed by polishing with CMP (chemical mechanical polishing) polishing techniques

Metallographic microstructure of alumina
Metallographic microstructure of ALON or alumina / aluminum nitride
Metallographic microstructure of Mullite
Metallographic microstructure of Steatite
Metallographic microstructure of berillium oxide