| Etchant | Conc. | Conditions | Comments |
|---|---|---|---|
|
Nital:
Ethanol Nitric acid |
100 ml 1-10 ml |
Seconds to minutes | Do not exceed 10% nitric acid -explosive |
|
KLEMMS 2:
Saturated sodium thiosulfate Potassium metabisulfite |
250 ml 25 grams |
Seconds to minutes | Dual phase tint etchant. Ferrite is light or dark blue, martensite brown and black, retained austenite white. Heating to 40°C will enhance the staining |
![]() |
| Nodular Cast Iron, 2% Nital,, 100X (DIC) |
![]() |
| Gray Cast Iron, Klemms 2 tint etch, 40°C, 1000X (BF). Blue is ferrite, brown is martensite, austenite is white |