Description:

CERMETS are a class of very hard and tough materials which combine the hardness of ceramics with the toughness of very wear resistant metals. Tungsten Carbide grinding drill bits is a primary example of a CERMET. Specimen preparation of these materials requires diamond grinding and polishing abrasives.

Preparation Challenge:

Proper specimen preparation requires that grinding damage be minimized as early as possible followed by polishing with CMP (chemical mechanical polishing) polishing techniques.

Examples:
CERMET PROCEDURES
Tungsten Carbide
PACE Technologies metallographic specimen preparation of CERMET's such as tungsten carbide


Copyright 2006-2024
PACE TECHNOLOGIES® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved

PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos