Hastelloy etched with Adlers etchant, Mag. 200X (DIC). Composition: Molybdenum: 8-10%, Chromium: 20.5-23%, Iron: 17-20%, Tungsten: 0.2-1%, Cobalt: 0.5-2.5%, Carbon: 0.05-.015%, Silicon: 1%, Manganese: 1%, Boron: 0.01%, Phosphorus: 0.04%, Sulfur: 0.03%, Nickel: Remainder |
CAUTION:Safety is very important when etching. Be sure to wear the appropriate protective clothing and observe all WARNINGS on chemical manufacuters SDS (Safety Data Sheets). Also review the COMMENTS and CONDITIONS Section for each etchant.