30 um Diamond Lapping Film*
|
POLYLUBE Diamond
Extender |
5-10 lbs |
200/200 rpm |
Planar
|
|
 |
15 um Diamond Lapping Film*
|
POLYLUBE Diamond
Extender |
5-10 lbs |
200/200 rpm |
3 min |
 |
 |
9 um Diamond Lapping Film*
|
POLYLUBE Diamond
Extender |
5-10 lbs |
200/200 rpm |
2 min |
 |
 |
6 um Diamond Lapping Film*
|
POLYLUBE Diamond
Extender |
5-10 lbs |
200/200 rpm |
2 min |
 |
 |
3 um Diamond Lapping Film*
|
POLYLUBE Diamond
Extender |
5-10 lbs |
200/200 rpm |
2 min |
 |
 |
1 um DIAMAT diamond
on ATLANTIS polishing pad |
DIALUBE Purple
Lubricant |
5-10 lbs |
200/200 rpm |
1 min |
 |
 |
MICROPAD or MICROPAD 2
polishing pad |
Colloidal silica |
5-10 lbs |
200/200 rpm |
30 sec |
 |
 |