The microstructure of thermal spray coatings has found applications in the medical as well as the aerospace industry.
Preparation Challenge: Keeping in mind that thermal spray coatings have basically been applied in order to modify a materials surface properties; the challenge in microstructural preparation of these materials is to maintain both their flatness and structural integrity.
| THERMAL SPRAY PROCEDURES | |
|---|---|
Nickel Chrome Coatings![]() |
Zirconia Coating on
Nickel Superalloy![]() |
Tungsten-Cobalt Coating![]() |
Nickel-Aluminum-Moly
Coating ![]() |
Nickel-Aluminum Coating ![]() |
|