METALLOGRAPHIC BRINELL HARDNESS TESTING VIDEO'S

Brinell OMEGA-HB-3000 Hardness Tester
Metallographic Brinell Hardness Tester BRN-3000 Brinell Hardness Tester

Return to top

Click here to get a quote METALLOGRAPHIC BRINELL HARDNESS TESTERS SPECIFICATIONS
Feature OMEGA-HB OMEGA-HB-3000 OMEGA-AUTO-HB
Measuring range 8 to 650 HBW 62.5, 100, 125, 187.5,
250, 500, 750, 1000, 1500, 3000
62.5, 100, 125, 187.5,
250, 500, 750, 1000, 1500, 3000
Test forces 187.5, 250, 500, 750,
1000, 3000 Kgf
~8 to 650 HBW ~8 to 650 HBW
Max Height of Specimen n/a 8.8-inch (225 mm) 10 inches (260 mm)
Instrument Throat Height n/a 5.3-inch (135 mm) 6 inches (150 mm)
Electrical Requirements Manual 110 or 220V 110 or 220V
Dimensions (W x D x H) Manual 9.3 x 21.5 x 31.1-inch
(235 x 5450 x 790 mm)
12 x 24.5 x 39 inches
(313 x 622 x 992 mm)
Weight 420 lbs (210 kg) 290 lbs (130 kg 200 lbs (170 kg)
Optical measuring device (sold separately) BrinScan Measuring System Built-in Built-in

Return to top

Click here to get a quote METALLOGRAPHIC MACROVICKERS HARDNESS TESTER SPECIFICATIONS
Feature OMEGA-5000-HZ MacroVickers
Test Force 1kgf, 2kgf, 2.5kgf, 3kgf, 5kgf,
10kgf, 20kgf, 30kgf, 50kgf
Eyepieces 10X
Objective 10X, 20X
Total Magnification 100X, 200X
Loading Method Automatic
(Loading/Dwell/Unloading)
Dwell time Adjustable 5-60 seconds
Shifting between
Objective and Indenter
Automatic Shifting
Resolution 0.25µm ,0.125µm
Illumination Halogen
Maximum Sample Height 6.7-inch (170 mm)
Throat Height 6.7-inch (5.1 mm)
Power 110 or 220V
Dimensions (W x D x H) 11 x 21 x 25 inch
(280 x 530 x 630mm)
Weight 77 lbs (35 kg)
Standards ISO 6507,ASTM E92,
JIS Z2244,GB/T 4340.2

Return to top

Copyright 2006-2021
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved


PACE Technologies facebook link Blog us on Tumblr Blog us on Tumblr PACE Technologies LinkIn PACE Technologies YouTube Videos