PACE Technologies logo PACE Technologies web collage PACE Technologies best price guarantee logo



Click here to get a quote

METALLOGRAPHIC VIBRATORY POLISHER VIDEO'S

GIGA Vibratory Polisher
GIGA Metallographic Vibratory Polisher

Return to top

Click here to get a quote

Metallographic Vibratory Polisher Specifications

Feature Specification
Polishing Bowl size 12-inch diameter
Drive Mechanism Horizontal frequency control, speed variable voltage control
Construction Aluminum casting, FRP (reinforced plastic) cover and acrylic hood
Electrical Specifications 110V or 220V 50/60 Hz
Construction Aluminum casting with GRP (glass reinforced plastic)
Frequency 1-240 Hz
Variable Voltage (speed controller) 1-200 volts
Dimensions
(W x D x H)
660 mm x 430 mm x 530 mm
26 x 17 x 21-inches
Weight 285 lbs (135 kgs)
Part No. GIGA-1200
Fixtures GIGA fixtures

Return to top

Copyright 2006-2021
PACE Technologies ® - 3601 E. 34th St., Tucson, AZ 85713, USA
Telephone +1-520-882-6598 FAX +1-520-882-6599
All Rights Reserved